公开(公告)号:DE3367397D1
公开(公告)日:1986-12-11
申请号:DE3367397
申请日:1983-06-20
Applicant: BASF AG
Inventor: ZEITLER GERHARD DR , WERNER FRANK DR , BITTNER GERHARD DR , BAUMANN KARL-HEINZ DR , ROEBER ARTUR , METZINGER LOTHAR DR , OHLINGER RAINER DR , ZETTLER HANS DIETER
Abstract: In order to prepare thermoplastic polyurethane elastomers (a) organic diisocyanate, (b) polyhydroxyl compounds with molecular weights of 500 to 8,000, and (c) chain extenders with molecular weights of 60 to 400 in the presence of (d) catalysts, and optionally (e) auxiliaries, and/or (f) additives are reacted in two reaction stages at temperatures from 60 DEG C. to 250 DEG C. In the first reaction stage the components are continuously mixed, the reaction mixture is applied to a carrier, preferably a conveyor band of thermoplastic material, and is allowed to react at the reaction temperature until solidified. Subsequently, the solidified reaction mixture is melted in an extruder and the reaction is completed in the second reaction stage.
-
公开(公告)号:AT23345T
公开(公告)日:1986-11-15
申请号:AT83105994
申请日:1983-06-20
Applicant: BASF AG
-
公开(公告)号:DE3301345A1
公开(公告)日:1984-07-19
申请号:DE3301345
申请日:1983-01-18
Applicant: BASF AG
Inventor: FISCHER JUERGEN DR , SEILER ERHARD DR , ROEBER ARTUR , HEYM MANFRED DR , NEITZEL MANFRED PROF DR
-
公开(公告)号:DE3381557D1
公开(公告)日:1990-06-21
申请号:DE3381557
申请日:1983-07-11
Applicant: BASF AG
Inventor: HORN PETER DR , GEHM ROBERT DR , MARX MATTHIAS DR , ROEBER ARTUR
-
公开(公告)号:CA1254455A
公开(公告)日:1989-05-23
申请号:CA514501
申请日:1986-07-23
Applicant: BASF AG
Inventor: FISCHER JUERGEN , ROEBER ARTUR
Abstract: PROCESS AND DEVICE FOR THE PREPARATION OF FIBER COMPOSITE MATERIALS Summary A continuous process for the preparation of fiber composite materials by impregnating fiber reinforcing material with a solution of a thermoplastic or thermosetting plastic precursor, followed by evaporating the solvent used by means of exposure to light having a wave length corresponding to the absorption maximum of the solvent.
-
公开(公告)号:DE3376060D1
公开(公告)日:1988-04-28
申请号:DE3376060
申请日:1983-11-28
Applicant: BASF AG
Inventor: HORN PETER DR , ROEBER ARTUR , MARX MATTHIAS DR , SEILER ERHARD DR , NISSEN DIETMAR DR , HEYM MANFRED DR , FISCHER JUERGEN DR
-
公开(公告)号:DE3224324A1
公开(公告)日:1984-01-05
申请号:DE3224324
申请日:1982-06-30
Applicant: BASF AG
Inventor: ZEITLER GERHARD DR , WERNER FRANK DR , BITTNER GERHARD DR , BAUMANN KARL-HEINZ DR , ROEBER ARTUR , METZINGER LOTHAR DR , OHLINGER RAINER DR , ZETTLER HANS DIETER DIPL ING
Abstract: In order to prepare thermoplastic polyurethane elastomers (a) organic diisocyanate, (b) polyhydroxyl compounds with molecular weights of 500 to 8,000, and (c) chain extenders with molecular weights of 60 to 400 in the presence of (d) catalysts, and optionally (e) auxiliaries, and/or (f) additives are reacted in two reaction stages at temperatures from 60 DEG C. to 250 DEG C. In the first reaction stage the components are continuously mixed, the reaction mixture is applied to a carrier, preferably a conveyor band of thermoplastic material, and is allowed to react at the reaction temperature until solidified. Subsequently, the solidified reaction mixture is melted in an extruder and the reaction is completed in the second reaction stage.
-
公开(公告)号:AT52744T
公开(公告)日:1990-06-15
申请号:AT83106769
申请日:1983-07-11
Applicant: BASF AG
Inventor: HORN PETER DR , GEHM ROBERT DR , MARX MATTHIAS DR , ROEBER ARTUR
-
公开(公告)号:CA1225189A
公开(公告)日:1987-08-04
申请号:CA430955
申请日:1983-06-22
Applicant: BASF AG
Inventor: ZEITLER GERHARD , WERNER FRANK , BITTNER GERHARD , BAUMANN KARL-HEINZ , ROEBER ARTUR , METZINGER LOTHAR , OHLINGER RAINER , ZETTLER HANS D
Abstract: TWO-STACE PROCESS FOR THE PREPARATION OF THERMOPLASTIC POLYURETHANE ELASTOMERS In order to prepare thermoplastic polyurethane elastomers a) organic diisocyanate, b) polyhydroxyl compounds with molecular weights of 500 to 8,000, and c) chain extenders with molecular weights of 60 to 400 in the presence of d) catalysts, and optionally e) auxiliaries, and/or f) additives are reacted in two reaction stages at temperatures from 60.degree.C to 250.degree.C. In the first reaction stage the components are continuously mixed, the reaction mixture is applied to a carrier, preferably a conveyor band of thermoplastic material, and is allowed to react at the reaction temperature until solidified. Suhsequently, the solidified reaction mixture is melted in an extruder and the reaction is completed in the second reaction stage.
-
公开(公告)号:CA1193399A
公开(公告)日:1985-09-10
申请号:CA432865
申请日:1983-07-21
Applicant: BASF AG
Inventor: HORN PETER , GEHM ROBERT , MARX MATTHIAS , ROEBER ARTUR
IPC: C01B33/32 , C08G18/00 , C08G18/18 , C08G18/32 , C08G18/38 , C08G18/50 , C08G18/83 , C08G77/02 , C08K3/34 , C08G18/14 , C08G18/40 , C08J9/04
Abstract: Stable water glass solutions are obtained (A) by mixing a solution of an aqueous alkali silicate solution and alkali hydroxide with a tertiary amine and subsequently oxyalkylating the resultant two-phase reaction mixture with at least one alkylene oxide in such an amount that a uniform solution forms or (B) by oxyalkylating a tertiary amine with at least one alkylene oxide and mixing the resultant reaction mixture with a solution of an aqueous alkali silicate solution and alkali hydroxide. The stable water glass solutions are suitable for the preparation of organo silicate foams. For the preparation of the organo silicate foams, a mixture of the stable water glass solutions and tertiary amino group-containing polyether polyols is reacted with organic polyisocyanates in the presence of catalysts, blowing agents and optionally auxiliaries and additives.
-
-
-
-
-
-
-
-
-