WATER-MAKING APPARATUS AND METHOD THEREFOR

    公开(公告)号:JPH1190429A

    公开(公告)日:1999-04-06

    申请号:JP25317797

    申请日:1997-09-18

    Abstract: PROBLEM TO BE SOLVED: To provide a water producing apparatus which easily, quickly, and reliably produces drinking water and water for household use even in a site where water supply is not available and make the apparatus light weight, compact, and economical by installing an electric motor using a storage battery as an electric power source, a raw water pump employing the electric motor as a driving source, and a separation membrane module unit. SOLUTION: A cable 22 is connected with a storage battery 21 of a vehicle 40, a strainer 1 connected with a raw water hose 3 is placed in a lake or a marsh or a river, a prime motor of the vehicle 40 is started, a raw water pump 7 is driven by an electric motor 6, and water is sent to a prefilter 9 through the strainer 1. The water is pre-treated to remove SS components and sent to a reverse osmosis membrane module unit 11 to remove dissolved, components such as salts, trihalomethane, and the likes contained in the water passed through the unit. A part of the obtained water is discharged to outside through a concentrated water distributing pipe 12 to be used for household use. The remaining water is sent to an aspirator 17 after being passed through a filtered water distributing pipe 14, a soluble disinfectant in a disinfectant bottle 20 is added to water when the water flows by, and the water is disinfected and discharged as drinking water to outside.

    PREPARATION OF COMPOSITE MEMBRANE FOR REVERSE OSMOSIS

    公开(公告)号:JPS5864102A

    公开(公告)日:1983-04-16

    申请号:JP16096081

    申请日:1981-10-12

    Abstract: PURPOSE:To stabilize membrane properties, in preparing a composite membrane for reverse osmosis, by permitting a definite amount of an org. solvent for a porous support present in a membrane forming solution and/or water contained in said porous support. CONSTITUTION:In preparing a composite membrane for reverse osmosis by a method wherein a membrane forming solution (pref., a monomer coating polymerizable solution consisting of, for example, furfuryl alcohol, isocyanuric acid and sulfuric acid as a catalyst) is coated on a porous support comprising porous polysulfone or the like in a wet state and heat treatment is subsequently carried out at 100-170 deg.C, an org. solvent for said support (DMF or DMSO) is made present in a range shown by a formula 0.1

    POLYOLEFIN-BASED CROSSLINKED FOAM

    公开(公告)号:JPH11228725A

    公开(公告)日:1999-08-24

    申请号:JP4288698

    申请日:1998-02-09

    Abstract: PROBLEM TO BE SOLVED: To obtain a polyolefin-based foam having good whiteness without generating environmental health problems by maintaining and stabilizing whiteness and overcoming polymer degradation caused by high-temperature treatments. SOLUTION: In a sheet polyolefin-based crosslinked foam, a composite blowing agent of azodicarbonamide (A) and N,N'-dinitrosopentamethylenetetramine (B) blended in a ratio of (B)/[(A)+(B)] of 0.1-5 is concurrently used together with a mixed heat stabilizer of a hindered phenol-based and a thio-based stabilizers.

    CROSSLINKED POLYPROPYLENE-BASED FOAMED RESIN COMPOSITION AND CROSSLINKED FOAMED SHEET

    公开(公告)号:JPH11228721A

    公开(公告)日:1999-08-24

    申请号:JP4440998

    申请日:1998-02-10

    Abstract: PROBLEM TO BE SOLVED: To obtain a resin composition for foaming and which is excellent in formability, mechanical strength, elongation, thermal stability, or the like, and to provide a foamed body therefrom. SOLUTION: A crosslinked polypropylene-based foamed resin composition comprises 1-10 pts.wt. of a bifunctional vinyl group-containing benzene compound (c) which has a content (M) of a benzene compound having a vinyl group located at a para position of 0.18-0.69, 0.5-5 pts.wt. of an alkyl group and monofunctional vinyl group-containing benzene compound (d) and 1-10 pts.wt. of a thermally decomposable chemical foaming agent per 100 pts.wt. as the sum of 50-90 wt.% of a polypropylene resin (a) having an MFR of 0.5-10 g/10 min. and 10-50 wt.% of a polyethylene-based resin (b) having an MFR of 1-30 g/10 min.

Patent Agency Ranking