Method of working a work piece with a coating of a lignin-derived substance, wooden element with a coating of such lignin-derived substance, and structures, interior or exterior, with such wooden element
    85.
    发明授权
    Method of working a work piece with a coating of a lignin-derived substance, wooden element with a coating of such lignin-derived substance, and structures, interior or exterior, with such wooden element 有权
    用木质素衍生物质的涂层,具有这种木质素衍生物质的涂层的木质元件以及内部或外部的这种木质元件的结构来加工工件的方法

    公开(公告)号:US09205457B2

    公开(公告)日:2015-12-08

    申请号:US13824213

    申请日:2011-09-15

    Applicant: Leif Hansen

    Inventor: Leif Hansen

    Abstract: The invention relates to a method of working the surface of an edge or pattern on a work piece made, at least partly, of a wooden material. The method comprising a primary production step of processing the work piece by shaping said edge or pattern on the work piece. The primary production step further comprises applying a coating of phenylpropanoid polymer to said shaped edge or pattern, said coating being a surplus to any phenylpropanoid polymer present in the wooden material before applying the coating, and heating and mechanically working said edge or pattern, resulting in respectively the coating of phenylpropanoid polymer hardening during polymerization and a finished surface of said edge or pattern on the work piece.

    Abstract translation: 本发明涉及一种在至少部分由木质材料制成的工件上加工边缘或图案的表面的方法。 该方法包括通过使工件上的所述边缘或图案成形来加工工件的主要生产步骤。 初级生产步骤还包括将苯丙素类聚合物的涂层施加到所述成形边缘或图案,所述涂层在施加涂层之前是木质材料中存在于任何苯丙素类聚合物的剩余物,并加热和机械加工所述边缘或图案,导致 分别在聚合期间固化苯丙素聚合物的涂层和工件上的所述边缘或图案的成品表面。

    Rapid action coater
    87.
    发明申请
    Rapid action coater 审中-公开
    快速涂布机

    公开(公告)号:US20090196991A1

    公开(公告)日:2009-08-06

    申请号:US11630966

    申请日:2005-08-15

    Abstract: A new device and process for continuously applying coatings, such as resin and additives or polymers or the like, to minerals is disclosed. The device and apparatus differ substantially from standard batch coating processes currently used by industry. The apparatus uses a horizontal cylinder with an internal auger and a series of injection ports distributed along the cylinder. Minerals that are to be coated are pretreated and passed through the mixing cylinder using the auger (which may comprise one or more screws with variable pitch blades). As the mineral particles pass through the cylinder various coating materials are injected by the injection ports. The complete system is described, the method of use is explained and the control system which allows for different products is described.

    Abstract translation: 公开了一种用于将诸如树脂和添加剂或聚合物等的涂料连续施用于矿物的新装置和方法。 该装置和装置与工业目前使用的标准批量涂布方法有很大不同。 该装置使用具有内部螺旋推运器的水平气缸和沿气缸分布的一系列喷射口。 要涂覆的矿物被预处理并通过螺旋钻(其可以包括具有可变节距叶片的一个或多个螺钉)通过混合筒。 当矿物颗粒通过气缸时,各种涂料通过注射口注入。 描述了完整的系统,并说明了使用方法,并描述了允许不同产品的控制系统。

    Sealing Film and a Semiconductor Device Using the Same
    88.
    发明申请
    Sealing Film and a Semiconductor Device Using the Same 失效
    密封膜和使用其的半导体器件

    公开(公告)号:US20090189300A1

    公开(公告)日:2009-07-30

    申请号:US12299714

    申请日:2008-01-24

    Abstract: The present invention provides a sealing film excellent in filling properties and adhesiveness as a sealing film which comprises a resin layer containing the following (A), (B) and (C) and having a flow within the range of 150 to 1800 μm at 80° C.: (A) a resin component containing (a1) a high-molecular-weight component comprising crosslinking functional groups and having a weight-average molecular weight of 100,000 or more and a Tg within the range of −50 to 50° C. and (a2) a thermoplastic component comprising an epoxy resin as main component, (B) a filler having an average particle size within the range of 1 to 30 μm, and (C) a colorant, as well as a method for manufacturing the same and a semiconductor device using the same. The present invention also provides a sealing film excellent in adhesiveness and shape retention as a sealing film which comprises a resin layer containing the above (A), (B) and (C) and having a resin layer having a viscosity within the range of 10000 to 100000 Pa·s in a B-stage state at 50 to 100° C. in thermosetting viscoelasticity measurement, as well as a semiconductor device using the same.

    Abstract translation: 本发明提供作为密封膜的填充性和密合性优异的密封膜,该密封膜包含含有下述(A),(B)和(C)的树脂层,并且在80℃下流动在150〜1800μm的范围内 ℃:(A)含有(a1)包含交联官能团并且重均分子量为100,000以上且Tg在-50〜50℃的范围内的高分子量成分的树脂成分 和(a2)包含环氧树脂作为主要成分的热塑性组分,(B)平均粒度在1至30μm范围内的填料和(C)着色剂,以及制备 相同的半导体器件和使用其的半导体器件。 本发明还提供了作为密封膜的粘合性和形状保持性优异的密封膜,其包含含有上述(A),(B)和(C)的树脂层,并且具有粘度在10000以下的树脂层 在50〜100℃的B阶状态下,在热固性粘弹性测定中为100000Pa.s,以及使用其的半导体装置。

    Process for treating wood and products
    89.
    发明申请
    Process for treating wood and products 审中-公开
    木材和制品的处理

    公开(公告)号:US20050153152A1

    公开(公告)日:2005-07-14

    申请号:US11005479

    申请日:2004-12-07

    Applicant: Darrell Kelsoe

    Inventor: Darrell Kelsoe

    Abstract: Wood cellulose is treated with a reactive silicate. The reaction is done to cellulose within the wood and may be catalyzed with acid or base catalysts or a carbon silicon halogen combination which produces in situ acid catalysts or a different combination to produce an in situ base catalyst which replaces some of the molecules or atoms within the cellulose structure with silicon, boron or other hydrophobic or anti-degrading agents. Preferably an organic solvent, such as alcohol is used to accelerate the reaction with the water in the wood. Here, the hydroxyl (OH) group on some or all of the cellulose molecules is partially replaced with silicon or an alternative atom or molecule to changes the character of the wood. The process may be modified to insert a preliminary step of adding a reactive agent to be locked into the wood. Manufacturing techniques to enhance the process using ultrasound or other wave generating techniques are also taught.

    Abstract translation: 木纤维素用反应性硅酸盐处理。 对木材中的纤维素进行反应,并可用酸或碱催化剂或碳硅卤素组合催化,其产生原位酸催化剂或不同的组合以产生原位碱催化剂,其代替一些分子或原子 具有硅,硼或其它疏水或抗降解剂的纤维素结构。 优选地,使用诸如醇的有机溶剂来加速与木材中的水的反应。 这里,部分或全部纤维素分子上的羟基(OH)基团部分被硅或替代的原子或分子取代,以改变木材的性质。 可以修改该方法以插入将待锁定在木材中的反应剂添加的初步步骤。 还教导了使用超声或其他波浪生成技术来增强过程的制造技术。