Abstract:
A multilayer film comprising at least one core layer comprising a polypropylene composition comprising: A) from 95 wt% to 60 wt%; of a propylene homopolymer having a fraction insoluble in xylene at 25 °C greater than 90 wt%; and B) from 5 wt% to 40 wt%; of an heterophasic propylene ethylene copolymer: the sum of the amounts of A) and B) being 100.
Abstract:
A multilayer film is characterized by having at least a skin layer comprising a propylene -- ethylene copolymers characterized by the following features: ethylene derived units content of between 1.0 wt% and 15.0% wt%; molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; - the content of xylene soluble fraction (XS) and the ethylene derived units content (C2) fulfill the following relation: XS 0.435C2 where XS is the percentage by weight of the fraction soluble in xylene at 25°C and C2 is the percentage by weight of ethylene units in the said copolymers determined via NMR.
Abstract:
A propylene-1-hexene copolymer having: i) a content of 1-hexene derived units ranging from 0.6 wt% to 3.0 wt%; ii) melt flow rate (MFR) measured according to the method ISO 1133 (230° C, 5 kg) ranging from 0.5 g/10 min to 5.0 g/10 min iii) the polydispersity (PI) ranges from 4.5 to 10 and the distribution of molecular weight is of multimodal type; iv) the melting point ranges from 160°C to 145°C; v) the DSC curve (temperature/heat of fusion) shows at least two peaks.
Abstract:
A propylene ethylene copolymer characterized by the following features: - an ethylene content of between 1.0 and 4.0% by weight; - a molecular weight distribution (MWD), expressed in terms of Mw/Mn, of greater than 4.0; - a content of xylene soluble fraction (XS) and ethylene content (C2) that fulfills the following relationship: (C2x1.1)+1.25
Abstract:
A polypropylene composition comprising: A) from 50 wt% to 90 wt%; of a propylene homopolymer; B) from 10 wt% to 50wt%; of a copolymer of propylene with from 30.0 wt% to 70.0wt%, of ethylene derived units; the sum of the amount of component A) and B) being 100; the composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 2.2 and 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 0.5 to 100 g/10 min; iii) a xylene soluble fraction ranging from 20 wt% to 50 wt%; the polypropylene composition being obtained by a two steps polymerization process wherein the catalyst system contains bismuth.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the creep and recovery curve measured on the polymer fuse at 200°C measured according to the procedure reported in the characterizing section shows a maximum value between 600 and 1200 seconds lower than 53x10 -5 1/Pa.
Abstract:
Propylene-ethylene copolymers showing an ethylene content of between 0.1 and 10% by weight, a molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 3.0 and a content of xylene soluble fraction (XS) and ethylene content (C2) such that the point defined by said values falls below the line given by the equation XS= 1.0296 . e 0.435C2 show high transparency and low melting temperature.
Abstract:
Extruded or molded profiles comprising a polyolefin composition consisting of 85% by weight or more of a copolymer of 1-butene with ethylene (A) having an ethylene copolymerized content up to 18 % bymol, and having Mw/Mn lower than 3, hardness shore A (measured according to ISO 868) lower than 90, no melting point (TmII) detectable at the DSC after cancelling the thermal history, melting enthalpy (ΔHf), measured by DSC after 10 days of aging at room temperature,comprised between 4 and 15 J/g; and up to 15% by weight of a propylene copolymer or a composition of copolymers of propylene (B) having a melting point from about 26°C to 200°C, isotactic index greater than 90%.