公开(公告)号:DE59905186D1
公开(公告)日:2003-05-28
申请号:DE59905186
申请日:1999-02-05
Applicant: BASF AG
Inventor: SCHADE CHRISTIAN , FISCHER WOLFGANG , GAUSEPOHL HERMANN , JUENGLING STEPHAN , WARZELHAN VOLKER , FONTANILLE MICHEL , DEFFIEUX ALAIN , DESBOIS PHILIPPE
Abstract: Disclosed are a process for the preparation of an initiator composition comprising an alkali metal organyl and an aluminum organyl and a process for the polymerization of anionically polymerizable monomers.
-
公开(公告)号:DE59706702D1
公开(公告)日:2002-04-25
申请号:DE59706702
申请日:1997-12-01
Applicant: BASF AG
Inventor: JUENGLING STEPHAN , GAUSEPOHL HERMANN , WARZELHAN VOLKER , MCKEE EDMUND , FISCHER MICHAEL
IPC: C08L55/00 , C08F2/00 , C08F20/00 , C08F20/12 , C08F287/00 , C08F297/02 , C08L53/00
Abstract: Anionic polymerization is used for the preparation of reaction mixtures comprising homopolymers, copolymers or block copolymers, and of homopolymers, copolymers and block copolymers which comprise acrylates or methacrylates or acrylates and methacrylates, wherein olefinically unsaturated compounds which are not acrylate or methacrylate derivatives are employed as solvent or as solvent component.
-
公开(公告)号:DE59704476D1
公开(公告)日:2001-10-04
申请号:DE59704476
申请日:1997-10-21
Applicant: BASF AG
Inventor: JUENGLING STEPHAN , GAUSEPOHL HERMANN , WEISS HORST , BAUMGAERTEL MICHAEL
Abstract: Initiator systems for anionic polymerization of vinyl monomers with polar groups, containing A) a1) at least one starter having general formula R -M or R -M -RC, wherein R , R or R independently stand for branched or straight-chain alkyl radicals of 1-6 carbon atoms, aryl radicals of 6-20 carbon atoms or alkyl radicals with 1-6 carbon atoms carrying at least one phenyl radical and M stands for a metal selected from the group of alkaline metals, and M stands for a metal selected from the group of alkaline earth metals, or a2) as a starter "living" polymer chains, whose chain ends are possibly stabilized by sterically demanding and/or aromatic radicals and B) at least one alkaline (I) or alkaline earth metal alcoholate (II) or at least one alkaline (I) and at least one alkaline earth metal alcoholate (II) which have at least one amino or one phosphino substituent or at least one amino and one phosphino substituent.
-
公开(公告)号:AT361340T
公开(公告)日:2007-05-15
申请号:AT04820435
申请日:2004-12-14
Applicant: BASF AG
Inventor: STORK MARTIN , WEBER MARTIN , GOTTSCHALK AXEL , RIECHERS SVEN , GUENTHERBERG NORBERT , FISCHER WOLFGANG , LEBER LUDGER , ITTEMANN PETER , JUENGLING STEPHAN
IPC: C08F257/02 , C08F279/02 , C08F285/00 , C08L25/12 , C08L33/12 , C08L35/06 , C08L51/00 , C08L51/04 , C08L55/02
Abstract: The present invention relates to thermoplastic molding compositions comprising a mixture of (A) from 30 to 69% by weight, based on the sum of components (A), (B) and (C), of a methyl methacrylate polymer, (B) from 30 to 69% by weight, based on the sum of components (A), (B) and (C), of a copolymer obtainable by polymerizing a styrenic monomer and a vinyl cyanide, and (C) from 1 to 40% by weight, based on the sum of components (A), (B) and (C), of a graft copolymer obtainable from (C1) from 60 to 90% by weight, based on (C), of a core obtainable by polymerizing a 1,3-diene and a styrenic monomer, (C2) from 5 to 20% by weight, based on (C), of a first graft shell, and (C3) from 5 to 20% by weight, based on (C), of a second graft shell composed of an alkyl (meth)acrylate polymer, with the proviso that the ratio of (C2) to (C3) is in the range from 2:1 to 1:2.
-
公开(公告)号:DE10359358A1
公开(公告)日:2005-07-14
申请号:DE10359358
申请日:2003-12-16
Applicant: BASF AG
Inventor: STORK MARTIN , WEBER MARTIN , GOTTSCHALK AXEL , RIECHERS SVEN , GUENTHERBERG NORBERT , FISCHER WOLFGANG , LEBER LUDGER , ITTEMANN PETER , JUENGLING STEPHAN
IPC: C08F257/02 , C08F279/02 , C08F285/00 , C08L25/12 , C08L33/12 , C08L35/06 , C08L51/00 , C08L51/04 , C08L55/02 , C08L33/20 , C08L51/06 , C08J5/00
Abstract: The present invention relates to thermoplastic molding compositions comprising a mixture of (A) from 30 to 69% by weight, based on the sum of components (A), (B) and (C), of a methyl methacrylate polymer, (B) from 30 to 69% by weight, based on the sum of components (A), (B) and (C), of a copolymer obtainable by polymerizing a styrenic monomer and a vinyl cyanide, and (C) from 1 to 40% by weight, based on the sum of components (A), (B) and (C), of a graft copolymer obtainable from (C1) from 60 to 90% by weight, based on (C), of a core obtainable by polymerizing a 1,3-diene and a styrenic monomer, (C2) from 5 to 20% by weight, based on (C), of a first graft shell, and (C3) from 5 to 20% by weight, based on (C), of a second graft shell composed of an alkyl (meth)acrylate polymer, with the proviso that the ratio of (C2) to (C3) is in the range from 2:1 to 1:2.
-
公开(公告)号:DE50007302D1
公开(公告)日:2004-09-09
申请号:DE50007302
申请日:2000-05-11
Applicant: BASF AG
Inventor: JUENGLING STEPHAN , SCHADE CHRISTIAN , GAUSEPOHL HERMANN , WARZELHAN VOLKER , MOORS RAINER , SCHAECH HANSJOERG , QUEISSER JOACHIM , LUINSTRA GERRIT , DEMETER JUERGEN
IPC: C08F2/06 , C08F2/38 , C08F4/60 , C08F2/00 , C08F4/62 , C08F4/639 , C08F4/642 , C08F4/646 , C08F36/04 , C08F236/10 , C08F279/02 , C08F297/04 , C08L55/02
Abstract: In a process for polymerizing dienes in a solvent comprising vinylaromatic monomers, the polymerization is carried out in the presence of a metal compound of Ti, Zr, Hf, V, Nb, Ta, Cr, Mo or W as catalyst and a Lewis acid as cocatalyst and, if desired, an alkylating agent and, if desired, a regulator. This process can be used for preparing high-impact polystyrene, acrylonitrile-butadiene-styrene copolymers or methyl methacrylate-butadiene-styrene copolymers.
-
公开(公告)号:DE10019111A1
公开(公告)日:2001-10-25
申请号:DE10019111
申请日:2000-04-18
Applicant: BASF AG
Inventor: DEMETER JUERGEN , QUEISSER JOACHIM , LUINSTRA GERRIT , JUENGLING STEPHAN
IPC: C08F4/642 , C08F4/68 , C08F4/69 , C08F36/04 , C08F279/02 , C08L55/02 , C08F212/08 , C08F236/10
Abstract: A process for the polymerisation of dienes in a solvent containing vinyl-aromatic monomers is carried out in presence of an organometallic compound of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum or tungsten as catalyst, a Lewis acid cocatalyst and optionally an alkylating agent and/or a regulator. Independent claims are also included for: (a) production of high-impact polystyrene, acrylonitrile-butadiene-styrene copolymers or methyl methacrylate-butadiene-styrene copolymers using a rubber solution produced by the above process; (b) continuous production of impact-modified thermoplastic molding materials containing a rubber-based soft phase dispersed in a hard vinyl-aromatic matrix, by (1) polymerizing dienes in vinyl-aromatic monomer solution as above in a first reaction zone, (2) transferring the diene rubber to a second zone and subjecting it to anionic or radical polymerisation, optionally in presence of further vinyl-aromatic monomer or other comonomers in amounts sufficient to achieve phase inversion and (3) completing the polymerisation in a third zone with the amount of vinyl-aromatic monomer required for the impact-modified material.
-
公开(公告)号:DE59704039D1
公开(公告)日:2001-08-16
申请号:DE59704039
申请日:1997-11-28
Applicant: BASF AG
Inventor: MC KEE EDMUND , JUENGLING STEPHAN , WARZELHAN VOLKER , GAUSEPOHL HERMANN
IPC: C08L51/00 , C08F20/00 , C08F20/12 , C08F265/04 , C08F297/04
Abstract: Preparation of rubber-modified molding compositions comprisesa1) anionic polymerization of a mixture (A) comprising acrylate derivatives or methacrylate derivatives or acrylate derivatives and methacrylate derivatives and a solvent, if desired comprising olefinically unsaturated compounds which are not an acrylate derivative or a methacrylate derivative, ora2) sequential anionic polymerization of acrylate derivatives or methacrylate derivatives or acrylate derivatives and methacrylate derivatives in the presence of a solvent which, if desired, comprises olefinically unsaturated compounds to give block copolymers, andb) subjecting the reaction mixture obtained in a1) or a2) or a1) and a2) to a free-radical-initiated polymerization, if desired after the addition of unsaturated compounds.
-
公开(公告)号:DE19926283A1
公开(公告)日:2000-12-14
申请号:DE19926283
申请日:1999-06-09
Applicant: BASF AG
Inventor: JUENGLING STEPHAN , SCHADE CHRISTIAN , GAUSEPOHL HERMANN , WARZELHAN VOLKER
IPC: C08F12/04 , C08F36/04 , C08L55/02 , C08F4/52 , C08F297/04
Abstract: Solution polymerization of conjugated dienes in a vinyl aromatic compound is carried out using a lanthanide metal alkenyl complex and organoaluminum or boron co-catalyst. A process for the solution of conjugated dienes in a vinyl aromatic compound in the presence of a catalyst is claimed. The catalyst is prepared by reaction of an alkenyl complex of a lanthanide metal with a co-catalyst comprising: (A) an organoaluminum compound of formula (1)-(6); and (B) a boron compound of formula (7). AlR (1) HAlR (2) R AlOR (3) RAl(OR) (4) R Al(OAl(R))nOAlR (5) (OAl(R))n+2 (6) B(Y)p(C6H5-qR q)3-p (7) (DkH) (BYp(C6H5-qR q)4-p (8) R = 1-12C alkyl; n = 1-50; R = fluorine or 1-10C fluoroalkyl; Y = alkyl, C R 5, a sulfonate O3SR or O3SR , an amide NR 2, a pyridyl NC5R 5, a dipyridyl N2C10R 8, a pyrazolate N2C3R 3, a pyrazolylborate R B(N2C3R 3)3, a benzamidinate (R N)2CC6H5R , an alcoholate or phenolate OR , a siloxane OSiR 3, a thiolate SR , a cyclopentadienyl C5HrR 5-r, an indenyl C9H7-sR s, a fluorenyl C13H9-tR t, a phenyl C6HrR25-r, 1-20 C alkyl, alkenyl or alkinyl; R = H or 1-30C alkyl, 6-30C aryl or an optionally substituted silyl group; r,s = 0-5; t = 0-9; p = 0-2; q = 1-5; D = neutral donor ligand; k = 0-10.
-
公开(公告)号:DE19825485A1
公开(公告)日:1999-12-09
申请号:DE19825485
申请日:1998-06-08
Applicant: BASF AG
Inventor: MC KEE GRAHAM EDMUND , JUENGLING STEPHAN , WARZELHAN VOLKER , GAUSEPOHL HERMANN
IPC: C08L67/02 , C08L69/00 , C08F220/18 , C08J3/20 , C08J5/00 , C08J5/18 , C08L33/04 , C08L33/20 , D01F6/92
Abstract: Polymer mixtures, containing the following essential ingredients: A) 1-99 wt.% polycarbonates or polyester; B) 1-99 wt.% acrylate rubber modified moulding material, produced by b1) anionic polymerisation of monomers selected from the group consisting of i) (meth)acrylic acid esters of general formula (I) CH2=C(R )-CO2R , and ii) (meth)acrylic acid esters of general formula (II) CH2=C(R )-C(O)O-CR R R in a solvent containing vinyl aromatic compounds of general formula (III) and b2) by adding to the reaction mixture obtained according to b1) b21) acrylonitrile, methacrylonitrile, C1-C8 methacrylates or mixtures thereof and optionally, other radically polymerisable monomers selected from the group consisting of b22) vinyl aromatic compounds according to general formula (III), (C1-C8 alkyl) (meth)acrylic acid esters or the mixtures thereof, b23) other olefinically unsaturated compounds that are different from acrylonitrile or methacrylonitrile or vinyl aromatic compound (III), b3) radical polymerisation of the mixture obtained according to b2), in addition b4 to isolating the rubber modified moulding material obtained according to b3); C) 0-50 wt.% acrylate rubber modified moulding material, whereby at least the rubber phase is produced by means of emulsion polymerisation; D) 0-50 wt.% inorganic filler and E) 0-50 wt.% additives and auxiliary agents.
-
-
-
-
-
-
-
-
-