Abstract:
A propylene/ 1-hexene copolymer in which: i) the content of 1-hexene derived units, measured by C13-NMR, ranges from 1.5 wt% to 2.5 wt% and the content of propylene derived units ranges from 97.5 to 98.5 wt. %; ii) melting temperature measured by DSC in the range 148-153°C; iii) the amount of fraction insoluble in xylene at 25°C is higher than 97.0%; iv) has a melt flow rate (MFR) measured according to ISO 1133, 230°C, 2.16 kg ranging from 35 to 65 g/10 min. The copolymer is useful for the production of injection molded articles in particular Twin- Wall injection molding articles.
Abstract:
Cable insulation or jacketing comprising: from 20.0 wt% to 80.0 wt% of component T1) being an interpolymer of ethylene and less than 7 wt%, of one or more polymerizable comonomers; from 0.5 wt% to 5.0 wt% of a peroxide; from 20.0 wt% to 80.0 wt% of component T2) comprising A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 25-50% by weight; of a copolymer of ethylene and a C 3 -C 8 alpha-olefin containing from 0.1% to 20% by weight of alpha-olefin units; and C) 30-60% by weight of a copolymer of ethylene and propylene containing from 25% to 75% by weight of ethylene units.
Abstract:
A polyolefin composition comprising: T1) 70-95wt%, of a polyolefin component containing: a1) from 30 wt% to 70 wt% of a propylene based polymer; a2) from 30 wt% to 70 wt% of an ethylene based polymer; T2) 5-30 wt% of a polyolefin component containing: A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 25-50% by weight of a copolymer of ethylene and a C 3 -C 8 alpha-olefin comprising 0.1- 20% by weight of C 3 -C 8 alpha-olefin units; and C) 30-60% by weight of a copolymer of ethylene and propylene comprising 25-75% by weight of ethylene units.
Abstract:
Poliolefinic fiber comprising from 2wt% to 20 wt% relative to the total weight of the fiber of a polyolefin composition comprising: A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 25-50% by weight; of a copolymer of ethylene and a C 3 - C 8 alpha-olefin containing from 0.1% to 20% by weight of alpha-olefin units; and C) 30-60% by weight of a copolymer of ethylene and propylene containing from 25% to 75% by weight of ethylene units;
Abstract:
A propylene polymer composition comprising: a) from 35 wt% to 65 wt% of a propylene 1-hexene copolymer containing from 10.5 to 13.0% by weight, of 1-hexene derived units having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, i.e. at 230°C, with a load of 2.16 kg) from 3.5 to 12.0 g/10 min; b) from 35 wt% to 65 wt% of a propylene ethylene copolymer containing from 1.5 wt% to 6.wt% of ethylene derived units, a having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, i.e. at 230°C, with a load of 2.16 kg) from 3.5 to 12.0 g/10 min.
Abstract:
A film comprising a polypropylene composition comprising: A) from 50 wt% to 90 wt%; of a propylene homopolymer; B) from 10 wt% to 50wt%; of a copolymer of propylene with from 30.0 wt% to 70.0wt%, of ethylene derived units; the sum of the amount of component A) and B) being 100; the composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 2.2 and 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 0.5 to 50 g/10 min; iii) a xylene soluble fraction ranging from 20 wt% to 50 wt%; the polypropylene composition being obtained by a two steps polymerization process wherein the catalyst system contains bismuth.
Abstract:
The present invention concerns polypropylene compositions containing glass fiber fillers, having a high Melt Flow Rate (MFR) and a good balance of mechanical properties. In particular, the compositions of the present invention show excellent mechanical (high stiffness and ductility) and thermal properties (low shrinkage), while displaying a boost of the final MFR, notwithstanding the presence of glass fibers
Abstract:
A consumable filament for use in an extrusion-based additive manufacturing system comprising an heterophasic propylene ethylene copolymer having a xylene soluble content ranging from 1 wt% to 50 wt% and a melt flow rate MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) ranging from 0.5 to 100 g/10 min.
Abstract:
A plate for use in an extrusion-based additive manufacturing system comprising as a top layer a sheet or film comprising polyolefin composition A) wherein composition A) comprises: (i) 5-35% by weight; of a propylene homopolymer or a propylene ethylene copolymer (ii) 20-50% by weight; of a copolymer of ethylene and a C 3 -C 8 alpha-olefin; and (iii) 30-60% by weight of a copolymer of ethylene and propylene.
Abstract:
A polyolefin composition comprising: A) from 85.0 wt% to 99.5 wt%; of a propylene 1-hexene copolymer B) from 0.5 wt% to 15.0 wt%; of a propylene, ethylene copolymer composition comprising: b1) from 12 wt% to 52 wt%; of a propylene homopolymer or a propylene/ethylene copolymer b2) from 48 wt% to 88 wt% of a propylene ethylene copolymer having a content of ethylene derived units ranging from 15.0 wt% to wt% to 42.0 wt%; wherein the resulting polyolefin composition has an melt flow rate (230°C/5 kg.. ISO 1133) ranging from 0.2 g/lOmin to 4.0 g/10min; the sum A+B being 100 and the sum b1+b2 being 100.