51.
公开(公告)号:PL320223A1
公开(公告)日:1997-09-15
申请号:PL32022395
申请日:1995-06-27
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , BRUCHMANN BERND , BOECKH DIETER , SEELIGER URSULA , YAMAMOTO MOTONORI , BAUER PETER
IPC: C08J9/00 , A01G9/10 , C05F17/00 , C08G18/42 , C08G18/46 , C08G63/60 , C08G63/668 , C08G63/672 , C08G63/685 , C08G63/688 , C08G63/91 , C08L1/00 , C08L67/02 , C08L75/06 , C08L101/16 , C09J167/02 , C09J175/06 , C09K15/32
Abstract: Biodegradable polyether esters P1 obtainable by reacting a mixture essentially comprising(a1) a mixture essentially comprising20-95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof,5-80 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and0-5 mol % of a compound containing sulfonate groups,where the total of the individual mole percentages is 100 mol %, and(a2) a mixture of dihydroxy compounds essentially comprising(a21) from 15 to 99.8 mol % of a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols,(a22) from 85 to 0.2 mol % of a dihydroxy compound containing ether functionalities of the formula Iwhere n is 2, 3 or 4 and m is an integer from 2 to 250, or mixtures thereof,where the molar ratio of (a1) to (a2) is chosen in the range from 0.4:1 to 1.5:1, with the proviso that the polyether ester P1 has a molecular weight (Mn) in the range from 5000 to 80,000 g/mol, a viscosity number in the range from 30 to 450 g/ml (measured in o-dichlorobenzene/phenol (50/50 ratio by weight) at a concentration of 0.5% by weight of polyether ester P1 at 25° C.) and a melting point in the range from 50 to 200° C., and with the further proviso that from 0.01 to 5 mol %, based on the molar quantity of component (a1) employed, of a compound D with at least three groups capable of ester formation are employed to prepare the polyether ester P1,and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings and adhesives, biodegradable moldings, films and blends with starch obtainable from the polymers and molding compositions according to the invention.
-
公开(公告)号:NO973767D0
公开(公告)日:1997-08-15
申请号:NO973767
申请日:1997-08-15
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , PIPPER GUNTER , SEELIGER URSULA , BAUER PETER , PAGGA UDO , YAMAMOTO MOTONORI
IPC: C08G63/60 , C08J9/04 , C08G63/66 , C08G63/672 , C08G63/91 , C08L3/00 , C08L67/00 , C08L101/16 , C09J167/00 , D21H19/28 , C08G
Abstract: PCT No. PCT/EP96/00458 Sec. 371 Date Aug. 14, 1997 Sec. 102(e) Date Aug. 14, 1997 PCT Filed Feb. 3, 1996 PCT Pub. No. WO96/25448 PCT Pub. Date Aug. 22, 1996Biodegradable polymers comprising a polyether ester P1 obtained by reacting a first mixture of 20-95 mol% of adipic acid or ester-forming derivatives thereof or mixtures thereof, 5-80 mol% of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0-5 mol% of a compound containing sulfonate groups, and a second mixture of 15-99.8 mol% of a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, 85-0.2 mol% of a dihydroxy compound IHO-[(CH2)n-O]m-H(n=2, 3 or 4, m=2-250) with 0-5 mol%, based on the first mixture, of a compound D having at least three groups capable of ester formation, and a bisoxazoline C1, their preparation and their use in the manufacture of biodegradable molding materials.
-
公开(公告)号:NO972226A
公开(公告)日:1997-07-14
申请号:NO972226
申请日:1997-05-14
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , SCHORNICK GUNNAR , BRUCHMANN BERND , SEELIGER URSULA , YAMAMOTO MOTONORI , BAUER PETER
IPC: C08L3/00 , A01G13/02 , C08G18/42 , C08G18/46 , C08G18/66 , C08G63/00 , C08G63/183 , C08G63/20 , C08G63/60 , C08G63/688 , C08G63/91 , C08L3/02 , C08L67/02 , C08L75/06 , C08L101/16 , C09D167/00 , C09K17/52
CPC classification number: C08L3/02 , C08G18/4216 , C08G18/4219 , C08G18/4277 , C08G18/428 , C08G18/4286 , C08G18/4676 , C08G18/6659 , C08G63/20 , C08G63/60 , C08G2230/00 , C08L75/06 , C09D167/00 , C09K17/52 , Y02A40/284 , Y10S525/938 , Y10T428/31547 , Y10T428/31786 , Y10T428/31794 , C08L2666/02 , C08L2666/26 , C08L2666/36
Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd
-
公开(公告)号:FI972964A0
公开(公告)日:1997-07-11
申请号:FI972964
申请日:1997-07-11
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , SCHORNICK GUNNAR , BRAUN FRANK , SEELIGER URSULA , YAMAMOTO MOTONORI , BAUER PETER
IPC: C08G69/40 , C08G18/60 , C08G69/44 , C08G69/48 , C08G73/00 , C08G73/04 , C08J9/04 , C08K5/353 , C08L77/12 , C08L101/16 , C09J177/12 , D21H19/30 , C08G
Abstract: PCT No. PCT/EP96/00059 Sec. 371 Date Jul. 3, 1997 Sec. 102(e) Date Jul. 3, 1997 PCT Filed Jan. 9, 1996 PCT Pub. No. WO96/21690 PCT Pub. Date Jul. 18, 1996Biodegradable polyetheresteramides P1 which are obtained by reacting (a1) a mixture containing 20-95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof and 5-80 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and (a2) a mixture of dihydroxy compounds (a21) from 15 to 99.3 mol % of a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, (a22) from 0.2 to 85 mol % of a dihydroxy compound containing ether functionalities of the formula I HO-((CH2)n-O)m-H I where n is 2, 3 or 4 and m is an integer from 2 to 250, or mixtures thereof and (a23) from 0.5 to 80 mol % of an amino-C2-C12-alkanol or amino-C5-C10-cycloalkanol, where the molar ratio of (a1) to (a2) is from 0.4:1 to 1.5:1, with the proviso, inter alia, that the polyetheresteramides P1 have a molecular weight (Mn) in the range from 5000 to 80,000 g/mol, and biodegradable polymers, biodegradable moldings, and adhesives obtained from the disclosed polymers.
-
公开(公告)号:DE19505185A1
公开(公告)日:1996-10-24
申请号:DE19505185
申请日:1995-02-16
Applicant: BASF AG
Inventor: WARZELHAN VOLKER DR , PIPPER GUNTHER DR , SEELIGER URSULA DR , BAUER PETER , PAGGA UDO DR , YAMAMOTO MOTONORI
IPC: C08J5/00 , A61L15/26 , A61L15/62 , C08G63/183 , C08G63/20 , C08G63/60 , C08G63/668 , C08G63/672 , C08G63/688 , C08G63/91 , C08J9/00 , C08J9/04 , C08L67/00 , C08L101/16 , C09J167/00 , D21H19/28 , C08G63/16 , C08G63/40 , C08G63/685 , C08G81/00
Abstract: PCT No. PCT/EP96/00457 Sec. 371 Date Aug. 14, 1997 Sec. 102(e) Date Aug. 14, 1997 PCT Filed Mar. 5, 1996 PCT Pub. No. WO96/25446 PCT Pub. Date Aug. 22, 1996Biodegradable polyesters having a molecular weight (Mn) of from 5000 to 50,000 g/mol (measured by gel permeation chromatography), a viscosity number of from 30 to 350 g/ml (measured in 50:50 by weight of o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester at 25 DEG C.), and a melting point of from 50 to 170 DEG C., and having both hydroxyl and carboxyl end groups, the molar ratio of carboxyl end groups to hydroxyl end groups being greater than one, which is obtained by reacting a mixture consisting essentially of a1) a mixture consisting essentially of from 45 to 80 mol % of adipic acid or ester-forming derivatives thereof, or mixtures thereof, from 20 to 55 mol % of terephthalic acid or ester-forming derivatives thereof, or mixtures thereof, and from 0 to 5 mol % of a sulfonate compound, where the sum of the individual mole percentages is 100 mol %, and a2) a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, in the presence of from 0.01 to 5 mol %, per mol of component a1), of a compound D having at least three groups capable of ester formation, the molar ratio of a1) to a2) being from 0.4:1 to 1.5:1, polymers and biodegradable thermoplastic molding compositions, processes for their preparation and their use for producing biodegradable moldings, adhesives, foams and blends with starch obtained from the polymers or molding compositions.
-
56.
公开(公告)号:AU4717996A
公开(公告)日:1996-09-04
申请号:AU4717996
申请日:1996-02-03
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , PIPPER GUNTER , SEELIGER URSULA , BAUER PETER , BEIMBORN DIETER BERNHARD , YAMAMOTO MOTONORI
IPC: C08J9/04 , C08G63/60 , C08G63/66 , C08G63/672 , C08G63/91 , C08L3/00 , C08L67/00 , C08L101/16 , C09J167/00 , D21H19/28
Abstract: PCT No. PCT/EP96/00458 Sec. 371 Date Aug. 14, 1997 Sec. 102(e) Date Aug. 14, 1997 PCT Filed Feb. 3, 1996 PCT Pub. No. WO96/25448 PCT Pub. Date Aug. 22, 1996Biodegradable polymers comprising a polyether ester P1 obtained by reacting a first mixture of 20-95 mol% of adipic acid or ester-forming derivatives thereof or mixtures thereof, 5-80 mol% of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0-5 mol% of a compound containing sulfonate groups, and a second mixture of 15-99.8 mol% of a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, 85-0.2 mol% of a dihydroxy compound IHO-[(CH2)n-O]m-H(n=2, 3 or 4, m=2-250) with 0-5 mol%, based on the first mixture, of a compound D having at least three groups capable of ester formation, and a bisoxazoline C1, their preparation and their use in the manufacture of biodegradable molding materials.
-
公开(公告)号:AT122494T
公开(公告)日:1995-05-15
申请号:AT88120670
申请日:1988-12-10
Applicant: BASF AG
Inventor: SCHLAG JOHANNES DR , KOEHNLEIN ERNST DR , BAUER PETER , HERNER MARTIN DR , HUB HANS-HENNING DR
-
公开(公告)号:AT92503T
公开(公告)日:1993-08-15
申请号:AT87117074
申请日:1987-11-19
Applicant: BASF AG
Inventor: HASENBEIN NORBERT DR , BAUER PETER , SCHLEMMER LOTHAR , HAUSS ALFRED FRIEDRICH DR , GROPPER HANS DR , OHLINGER RAINER DR
IPC: C08F2/02 , C08F8/44 , C08F255/02 , C09J4/00 , C09J151/06
-
公开(公告)号:MX168439B
公开(公告)日:1993-05-25
申请号:MX392986
申请日:1986-10-02
Applicant: BASF AG
Inventor: BAUER PETER , HAUSZ ALFRED FRIEDRICH
-
公开(公告)号:DE3838492A1
公开(公告)日:1990-05-17
申请号:DE3838492
申请日:1988-11-12
Applicant: BASF AG
Inventor: SAIVE ROLAND DR , FUNK GUIDO DR , BAUER PETER , KONRAD RAINER DR
IPC: C08F2/14 , C08F2/34 , C08F4/68 , C08F6/00 , C08F6/06 , C08F6/08 , C08F8/00 , C08F10/02 , C08J3/00
Abstract: The invention relates to a process for the preparation of low- pressure ethylene polymers by polymerizing the monomers in the presence of a vanadium-containing Ziegler catalyst system, in which process the solid ethylene polymer obtained is reacted in the degassing zone with additives containing OH groups. The additives are preferably water or C1-C10-alcohols.
-
-
-
-
-
-
-
-
-