公开(公告)号:KR1020100038598A
公开(公告)日:2010-04-15
申请号:KR1020080097632
申请日:2008-10-06
IPC: B23K26/00 , B23K26/352 , B23K26/364
Abstract: PURPOSE: A surface processing method of sliding components for a vehicle is provided to improve anti-scuffing property by splaying solid lubricant solution on the surface of the sliding components. CONSTITUTION: A surface processing method of sliding components for a vehicle comprises the following steps. A laser surface micromachining is enabled on the surface of an engine sliding component to form a dimple. The solid lubricant solution is sprayed on the surface of the sliding components to be fixed on the surface of the sliding components. A laser surface micromachining process enabled on a pulsed mode.
Abstract translation: 目的:提供用于车辆的滑动部件的表面处理方法,以通过在滑动部件的表面上张开固体润滑剂溶液来改善抗磨损性能。 构成:用于车辆的滑动部件的表面处理方法包括以下步骤。 在发动机滑动部件的表面上实现激光表面微加工以形成凹坑。 将固体润滑剂溶液喷涂在滑动部件的表面上以固定在滑动部件的表面上。 在脉冲模式下启用激光表面微加工工艺。
-
公开(公告)号:KR100992666B1
公开(公告)日:2010-11-05
申请号:KR1020080088932
申请日:2008-09-09
Applicant: 현대자동차주식회사 , 충남대학교산학협력단
Abstract: 본 발명은 생분해성 콩단백질/천연섬유 복합재 및 이의 제조방법에 관한 것으로서, 더욱 상세하게 설명하면, 생분해 특성이 우수한 콩단백질 등을 함유하는 매트릭스 수지와 단섬유, 직물 또는 부직포 형태의 천연섬유를 포함하는 생분해성 콩단백질/천연섬유 복합재 및 이의 제조방법에 관한 것이다. 본 발명의 콩단백질/천연섬유 복합재는 인장강도, 굽힘강도 등의 기계적 물성뿐만 아니라, 생분해성 역시 우수하여 매우 친환경적이다.
콩단백질, 생분해성, 복합재료-
公开(公告)号:KR101356176B1
公开(公告)日:2014-01-28
申请号:KR1020110087247
申请日:2011-08-30
IPC: G01N21/359 , G01N33/30
CPC classification number: G01N21/3577 , G01N21/359 , G01N33/2876 , G01N33/2888
Abstract: 파장 1000nm 이상의 근적외선을 이용하여 엔진오일의 1차 흡광도를 측정하는 1차측정단계; 상기 파장의 근적외선을 이용하여 사용중인 엔진오일의 2차 흡광도를 측정하는 2차측정단계; 및 상기 엔진오일의 2차 흡광도가 1차 흡광도에 비해 1.5배 이상의 증가율을 보일 때 엔진오일의 열화상태로 판단하는 비교단계;를 포함하는 엔진오일열화 감지방법 및 이를 위한 감지시스템이 소개된다.
-
公开(公告)号:KR1020100030138A
公开(公告)日:2010-03-18
申请号:KR1020080088932
申请日:2008-09-09
Applicant: 현대자동차주식회사 , 충남대학교산학협력단
Abstract: PURPOSE: A biodegradable soy protein/natural fiber composite is provided to ensure excellent tensile strength and flexural strength, to be biodegradable, and to be suitable as a material for exteriors of electronic parts or automobile interiors. CONSTITUTION: A biodegradable soy protein/natural fiber composite comprises a matrix resin containing soybean protein, plasticizer and cross-linking agent; a natural fiber selected from at least one or two kinds selected from jute, hemp, cotton fiber, coconut fiber, banana fiber, rice straw and wheat straw. The plasticizer is at least one or two kinds selected from glycerol, propandiol, polyethylene glycol and polyvinyl alcohol.
Abstract translation: 目的:提供可生物降解的大豆蛋白/天然纤维复合材料,以确保优异的抗拉强度和抗弯强度,可生物降解,并适合作为电子零件或汽车内饰外观的材料。 构成:可生物降解的大豆蛋白/天然纤维复合材料包含含有大豆蛋白,增塑剂和交联剂的基质树脂; 选自黄麻,大麻,棉纤维,椰子纤维,香蕉纤维,稻草和麦秆中的至少一种或两种的天然纤维。 增塑剂是选自甘油,丙二醇,聚乙二醇和聚乙烯醇中的至少一种或两种。
-
公开(公告)号:KR1020090106211A
公开(公告)日:2009-10-08
申请号:KR1020080031775
申请日:2008-04-04
IPC: G10K11/162 , G10K11/168 , B32B5/22 , B82Y30/00
CPC classification number: G10K11/168 , B32B5/22 , G10K2210/3223
Abstract: PURPOSE: An ultra-light sound-absorbing material and a manufacturing method including a nano fiber web are provided to selectively absorb specific frequency by combining main sound absorption factors. CONSTITUTION: An ultra-light sound-absorbing material and a manufacturing method including a nano fiber web are as follows. A hot air adhesive bonded non woven including average surface density includes the average surface density with 10~50 g/m. A composite film includes a first layer including the nano-fiber web and the first layer including the hot-air adhesive bonded non woven. The first layer with nano-fiber web is 0.9 ~ 10 mm.
Abstract translation: 目的:提供一种超轻型吸声材料和包括纳米纤维网的制造方法,以通过组合主要吸声因子来选择性地吸收特定频率。 构成:超轻型吸音材料及纳米纤维网的制造方法如下。 包含平均表面密度的非织造布热风粘合剂包括10〜50g / m 2的平均表面密度。 复合膜包括包括纳米纤维网的第一层和包含热粘合无纺布的热空气粘合剂的第一层。 具有纳米纤维网的第一层为0.9〜10mm。
-
公开(公告)号:KR1020130024051A
公开(公告)日:2013-03-08
申请号:KR1020110087247
申请日:2011-08-30
IPC: G01N21/359 , G01N33/30
CPC classification number: G01N21/3577 , G01N21/359 , G01N33/2876 , G01N33/2888
Abstract: PURPOSE: An engine oil deterioration sensing method and a system are provided to facilitate to determine the deterioration of engine oil by using a near-infrared measuring device which is cheap and possible to miniaturize, thereby enable to apply to a vehicle. CONSTITUTION: An engine oil deterioration sensing method is as follows. The primary absorbance of engine oil is measured by using near-infrared rays at a frequency of 100nm or greater. The secondary absorbance of the using engine oil is measured. A determination value multiplying a difference of the first absorbance and the second absorbance by the square of a daily mean driving distance is calculated. When the determination value is 500 or greater, the deterioration of the engine oil is determined.
Abstract translation: 目的:提供一种发动机油劣化检测方法和系统,以便于通过使用便宜且可能小型化的近红外测量装置来确定发动机油的劣化,从而能够应用于车辆。 构成:发动机油劣化检测方法如下。 发动机油的主要吸光度是通过使用频率为100nm以上的近红外线来测定的。 测量使用发动机油的二次吸光度。 计算将第一吸光度和第二吸光度的差乘以日平均驾驶距离的平方的确定值。 当判定值为500以上时,确定发动机油的劣化。
-
公开(公告)号:KR100962890B1
公开(公告)日:2010-06-10
申请号:KR1020070108626
申请日:2007-10-29
Applicant: 현대자동차주식회사 , 성균관대학교산학협력단
Abstract: 본 발명은 탄소나노튜브 강화 구리 복합재료의 제조방법에 관한 것으로서, 저밀도, 우수한 내부식성 및 내마모성, 우수한 휨 특성을 가지는 단일벽 탄소나노튜브에 니켈을 코팅하여 제조한 니켈 코팅된 탄소나노튜브를 구리 분말과 함께 분산용액에 투입하여 초음파 처리한 뒤 건조 및 소결 과정을 거쳐 제조함으로써, 고강도/고전도성의 탄소나노튜브 강화 구리 복합재료를 제조할 수 있는 니켈 코팅된 탄소나노튜브를 이용한 강화 구리 복합재료의 제조방법에 관한 것이다.
탄소나노튜브, 단일벽, 구리, 복합재료, 니켈, 고강도, 고전도성, 초음파 분산-
公开(公告)号:KR1020100025987A
公开(公告)日:2010-03-10
申请号:KR1020080084769
申请日:2008-08-28
Applicant: 현대자동차주식회사 , 인하대학교 산학협력단
Abstract: PURPOSE: A biodecomposable ABS/pulp composite material is provided to ensure mechanical properties such as tensile strength, tensile elongation ratio, and impact strength, and to be suitable for materials of automobile parts. CONSTITUTION: A biodecomposable ABS/pulp composite material comprises a matrix resin, an ethylene-propylene rubber grafted with maleic anhydride, and a styrene-acrylonitrile copolymer grafted with maleic anhydride. The matrix resin comprises an acrylonitrile-butadiene-styrene copolymer and pulp containing single or at least two kinds selected from needle-leaf kraft pulp, broadleaf kraft pulp and bleached pulp.
Abstract translation: 目的:提供一种生物可组合的ABS /纸浆复合材料,以确保机械性能如拉伸强度,拉伸伸长率和冲击强度,并适用于汽车部件的材料。 构成:生物可组合的ABS /纸浆复合材料包括基质树脂,接枝有马来酸酐的乙烯 - 丙烯橡胶和接枝马来酸酐的苯乙烯 - 丙烯腈共聚物。 基质树脂包括丙烯腈 - 丁二烯 - 苯乙烯共聚物和含有选自针叶牛皮纸浆,阔叶牛皮纸浆和漂白纸浆中的单一或至少两种的纸浆。
-
公开(公告)号:KR1020090032465A
公开(公告)日:2009-04-01
申请号:KR1020070097736
申请日:2007-09-28
Applicant: 현대자동차주식회사 , 연세대학교 산학협력단
Abstract: A method for bonding dissimilar aluminum using centrifugal casting is provided to produce products of high strength and abrasion-resistance while reducing the failure rate by making the cast structure fine. A method for bonding dissimilar aluminum using centrifugal casting comprises a first step of heating up the inner wall of a mold of a true-centrifugal caster, a second step of injecting molten metal to be used as an outer material into the mold, a third step of agitating while injecting molten metal to be used as an inner material into the mold, and a fourth step of cooling after hardening the molten metal.
Abstract translation: 提供了使用离心铸造来接合不同的铝的方法,以通过使铸造结构精细地降低故障率来生产高强度和耐磨性的产品。 使用离心铸造来接合不同的铝的方法包括:将真离心铸造机的模具的内壁加热的第一步骤,将用作外部材料的熔融金属注入模具的第二步骤,第三步骤 在将用作内部材料的熔融金属注入模具的同时搅拌,以及在熔融金属硬化后进行冷却的第四步骤。
-
公开(公告)号:KR101449045B1
公开(公告)日:2014-10-10
申请号:KR1020080084769
申请日:2008-08-28
Applicant: 현대자동차주식회사 , 인하대학교 산학협력단
Abstract: 본 발명은 생분해성 ABS/펄프 복합재료 및 이의 제조방법에 관한 것으로서, 더욱 상세하게 설명을 하면, 말레산무수물이 그라프트된 에틸렌-프로필렌 고무, 말레산무수물이 그라프트된 스타이렌-아크릴로니트릴 공중합체, 아크릴로니트릴-부타디엔-스타이렌 공중합체 및 펄프를 포함하는 복합재료에 관한 것이다. 본 발명의ABS/펄프 복합재료는 인장강도, 충격강도 및 내열변형성이 우수하여 전기전자기기용, 건축토목용 및 의료용 등의 부품, 특히 자동차 내장재로서 유용하게 사용될 수 있다.
아크릴로니트릴-부타디엔-스타이렌 공중합체, 말레산무수물
-
-
-
-
-
-
-
-
-