PROCESS FOR PRODUCING EXPANDABLE POLYLACTIC ACID-CONTAINING PELLETS

    公开(公告)号:CA3026811A1

    公开(公告)日:2017-12-14

    申请号:CA3026811

    申请日:2017-06-01

    Applicant: BASF SE

    Abstract: The invention relates to a process for producing expandable polylactic acid-containing pellets, comprising the steps of: a) melting and mixing in the following components: i) 65% to 95% by weight, based on the total weight of components i to iii, of polylactic acid, where the polylactic acid is composed of proportions of: ia) 65% to 95% by weight of polylactic acid having a D-lactic acid content of 0.3% to 5% by weight and ib) 5% to 3% by weight of polylactic acid having a D-lactic acid content of 10% to 18% by weight; ii) 15% to 35% by weight, based on the total weight of components i to iii, of an aliphatic polyester selected from the group consisting of polybutylene succinate, polybutylene succinate-co-adipate and polybutylene succinate-co-sebacate; iii) 0% to 2% by weight, based on the total weight of components i to iii, of a compatibilizer; iv) 0.1% to 5% by weight, based on the total weight of components i to iii, of an additive, b) mixing v) 1% to 7% by weight, based on the total weight of components i to iv, of an organic blowing agent and vi) 0.01% to 5% by weight of a co-blowing agent selected from the group of nitrogen, carbon dioxide, argon, helium and mixtures thereof into the polymer melt by means of a static or dynamic mixer at a temperature of at least 140°C, c) discharging through a die plate having bores having a diameter at the die exit of not more than 1.5 mm and d) pelletizing the blowing agent-containing melt directly beyond the die plate underwater at a pressure in the range from 1 to 21 bar.

    Método para producir granulados expandibles que contienen poli(ácido láctico)

    公开(公告)号:ES2581309T3

    公开(公告)日:2016-09-05

    申请号:ES13163665

    申请日:2011-01-06

    Applicant: BASF SE

    Abstract: Método para producir granulados expandibles que contienen poli(ácido láctico), el cual comprende las etapas de: a) fundir e incorporar en mezcla los componentes i) 50 a 99,9 % en peso, respecto del peso total de los componentes i a iii, de poli(ácido láctico), ii) 0 a 49,9 % en peso, respecto del peso total de los componentes i a iii, de uno o de varios otros polímeros iii) 0,1 a 2 % en peso, respecto del peso total de los componentes i a iii, de un diepóxido o poliepóxido y iv) 0,1 a 5 % en peso, respecto del peso total de los componentes i y iii, de un agente de nucleación, b) incorporar en mezcla v) 1 a 7 % en peso, respecto del peso total de los componentes i a iv, de un propelente orgánico y vi) 0,01 a 5 % en peso de un co-propelentes, que se selecciona del grupo de nitrógeno, dióxido de carbono, argón, helio o mezclas de los mismos, al polímero fundido por medio de un mezclador estático o dinámico a una temperatura de al menos 140 °C, c) descargar a través de una placa de toberas con perforaciones, cuyo diámetro a la salida de la tobera es de máximo 1,5 mm, y d) granular el material fundido que contiene propelente directamente después de la placa de toberas a una presión en el intervalo de 1 a 20 bar.

    Process for producing expandable polylactic acid-containing pellets

    公开(公告)号:AU2017276585B2

    公开(公告)日:2021-07-29

    申请号:AU2017276585

    申请日:2017-06-01

    Applicant: BASF SE

    Abstract: The invention relates to a process for producing expandable polylactic acid-containing pellets, comprising the steps of: a) melting and mixing in the following components: i) 65% to 95% by weight, based on the total weight of components i to iii, of polylactic acid, where the polylactic acid is composed of proportions of: ia) 65% to 95% by weight of polylactic acid having a D-lactic acid content of 0.3% to 5% by weight and ib) 5% to 3% by weight of polylactic acid having a D-lactic acid content of 10% to 18% by weight; ii) 15% to 35% by weight, based on the total weight of components i to iii, of an aliphatic polyester selected from the group consisting of polybutylene succinate, polybutylene succinate-co-adipate and polybutylene succinate-co-sebacate; iii) 0% to 2% by weight, based on the total weight of components i to iii, of a compatibilizer; iv) 0.1% to 5% by weight, based on the total weight of components i to iii, of an additive, b) mixing v) 1% to 7% by weight, based on the total weight of components i to iv, of an organic blowing agent and vi) 0.01% to 5% by weight of a co-blowing agent – selected from the group of nitrogen, carbon dioxide, argon, helium and mixtures thereof – into the polymer melt by means of a static or dynamic mixer at a temperature of at least 140°C, c) discharging through a die plate having bores having a diameter at the die exit of not more than 1.5 mm and d) pelletizing the blowing agent-containing melt directly beyond the die plate underwater at a pressure in the range from 1 to 21 bar.

    Process for producing expandable polylactic acid-containing pellets

    公开(公告)号:AU2017276585A1

    公开(公告)日:2019-01-03

    申请号:AU2017276585

    申请日:2017-06-01

    Applicant: BASF SE

    Abstract: The invention relates to a process for producing expandable polylactic acid-containing pellets, comprising the steps of: a) melting and mixing in the following components: i) 65% to 95% by weight, based on the total weight of components i to iii, of polylactic acid, where the polylactic acid is composed of proportions of: ia) 65% to 95% by weight of polylactic acid having a D-lactic acid content of 0.3% to 5% by weight and ib) 5% to 3% by weight of polylactic acid having a D-lactic acid content of 10% to 18% by weight; ii) 15% to 35% by weight, based on the total weight of components i to iii, of an aliphatic polyester selected from the group consisting of polybutylene succinate, polybutylene succinate-co-adipate and polybutylene succinate-co-sebacate; iii) 0% to 2% by weight, based on the total weight of components i to iii, of a compatibilizer; iv) 0.1% to 5% by weight, based on the total weight of components i to iii, of an additive, b) mixing v) 1% to 7% by weight, based on the total weight of components i to iv, of an organic blowing agent and vi) 0.01% to 5% by weight of a co-blowing agent – selected from the group of nitrogen, carbon dioxide, argon, helium and mixtures thereof – into the polymer melt by means of a static or dynamic mixer at a temperature of at least 140°C, c) discharging through a die plate having bores having a diameter at the die exit of not more than 1.5 mm and d) pelletizing the blowing agent-containing melt directly beyond the die plate underwater at a pressure in the range from 1 to 21 bar.

    Refuerzo con fibra de espumas reactivas a partir de un procedimiento de formación de espuma en molde

    公开(公告)号:ES2891775T3

    公开(公告)日:2022-01-31

    申请号:ES17723145

    申请日:2017-05-17

    Applicant: BASF SE

    Abstract: Artículo moldeado de espuma reactiva, caracterizado porque por lo menos una fibra (F) se encuentra con una zona (FB2) de la fibra dentro del artículo moldeado y está rodeado por la espuma reactiva, mientras una zona (FB1) de la fibra de la fibra (F) sobresale de un primer lado del artículo moldeado y una zona (FB3) de la fibra de la fibra (F) sobresale de un segundo lado del artículo moldeado, en donde la espuma reactiva es fabricada de acuerdo con un procedimiento de formación de espuma en molde, en donde la fibra (F) es introducida en la espuma reactiva en un ángulo α de 10 a 70° respecto a la dirección (d) de espesor del artículo moldeado y en donde el artículo moldeado es obtenible de acuerdo con un procedimiento que comprende las etapas a) a f): a) dado el caso aplicación de por lo menos una capa (S2) sobre por lo menos un lado de la espuma reactiva, b) generación de un orificio en cada fibra (F) en la espuma reactiva y dado el caso la capa (S2), en donde la perforación se extiende de un primer lado a un segundo lado de la espuma reactiva y dado el caso a través de la capa (S2), c) suministro de por lo menos una fibra (F) en el segundo lado de la espuma reactiva, d) paso de una aguja desde el primer lado de la espuma reactiva a través del orificio, hasta el segundo lado de la espuma reactiva y dado el caso paso de la aguja a través de la capa (S2), e) sujeción de por lo menos una fibra (F) mediante la aguja al segundo lado de la espuma reactiva, y f) retorno de la aguja junto con la fibra (F) a través del orificio, de modo que la fibra (F) se encuentra con la zona (FB2) de la fibra dentro del artículo moldeado y está rodeada por la espuma reactiva, mientras la zona (FB1) de la fibra de la fibra (F) sobresale de un primer lado del artículo moldeado o dado el caso de la capa (S2) y la zona (FB3) de la fibra de la fibra (F) sobresale de un segundo lado del artículo moldeado, en donde la totalidad de la superficie del artículo moldeado es cerrada en más de 30 %, determinado como se indica en la descripción indicada, en donde la espuma reactiva se basa en un poliuretano, una poliurea o un poliisocianurato, en donde el espesor del núcleo de la espuma reactiva aumenta hacia su superficie.

    Procedimiento para la producción de granulados expansibles conteniendo ácido poliláctico

    公开(公告)号:ES2854976T3

    公开(公告)日:2021-09-23

    申请号:ES17728499

    申请日:2017-06-01

    Applicant: BASF SE

    Abstract: Procedimiento para la producción de granulados conteniendo ácido poliláctico expansibles, comprendiendo los pasos: a) Fusión y mezcla de los componentes: i) del 65 al 95% en peso, relativo al peso total de los componentes i a iii, de ácido poliláctico, donde el ácido poliláctico consiste proporcionalmente en: ia) del 65 al 95 % en peso de ácido poliláctico con una proporción de ácido D-láctico del 0,3 al 5% y ib) del 5 al 35% en peso de ácido poliláctico con una proporción de ácido D-láctico del 10 al 18%; ii) del 5 al 35% en peso, relativo al peso total de los componentes i a iii, de un poliéster alifático seleccionado del grupo consistente en succinato de polibutileno, coadipato de succinato de polibutileno y cosebacato de succinato de polibutileno; iii) del 0 al 2% en peso, relativo al peso total de los componentes i a iii, de un compatibilizador; y iv) del 0,1 al 5 % en peso, relativo al peso total de los componentes i a iii, de un aditivo, b) Incorporación de v) del 1 al 7 % en peso, relativo al peso total de los componentes i a iv, de un propelente orgánico y vi) del 0,01 al 5 % en peso de un co-propelente - seleccionado del grupo nitrógeno, dióxido de carbono, argón, helio o mezclas de estos - en la masa fundida polimérica por medio de un mezclador estático o dinámico a una temperatura de al menos 140°C, c) descarga a través de una placa de boquillas con perforaciones, cuyo diámetro a la salida de boquilla asciende como máximo a 1,5 mm y d) granulación de la masa fundida conteniendo propelente directamente detrás de la placa de boquillas bajo el agua a una presión en el rango de 1 a 21 bar.

    Refuerzo con fibras de espumas de segmentos unidos entre sí

    公开(公告)号:ES2804105T3

    公开(公告)日:2021-02-03

    申请号:ES15813776

    申请日:2015-12-15

    Applicant: BASF SE

    Abstract: Cuerpo moldeado de espuma, donde la espuma comprende al menos dos segmentos de espuma unidos entre si, caracterizados porque al menos una fibra (F) esta ubicada con una region de fibra (FB2) dentro del cuerpo moldeado y esta encerrada por la espuma, mientras que una region de fibra (FB1) la fibra (F) sobresale de un primer lado del cuerpo moldeado y una region de fibra (FB3) de la fibra (F) sobresale de un segundo lado del cuerpo moldeado, en cuyo caso la fibra (F) ha sido parcialmente introducida mediante un procedimiento que comprende las siguientes etapas a) a f): a) dado el caso aplicar al menos una capa (S2) a al menos un lado de la espuma, b) generar un orificio por fibra (F) en la espuma y dado el caso en la capa (S2), en cuyo caso el orificio se extiende desde un primer lado a un segundo lado de la espuma y dado el caso a traves de la capa (S2), c) proporcionar al menos una fibra (F) en el segundo lado de la espuma, d) hacer pasar una aguja desde el primer lado de la espuma a traves del orificio hasta el segundo lado de la espuma, y dado el caso hacer pasar la aguja a traves de la capa (S2), e) fijar al menos una fibra (F) a la aguja en el segundo lado de la espuma, y f) devolver la aguja junto con la fibra (F) a traves del orificio, de modo que la fibra (F) este ubicada con la region de fibra (FB2) dentro del cuerpo moldeado y este encerrada por la espuma, mientras que la region de fibra (FB1) de la fibra (F) sobresale de un primer lado del cuerpo moldeado o dado el caso de la capa (S2) y la region de fibra (FB3) de la fibra (F) sobresale de un segundo lado del cuerpo moldeado.