METHOD FOR INCREASING THE MOLECULAR WEIGHT OF POLYESTERS
    1.
    发明申请
    METHOD FOR INCREASING THE MOLECULAR WEIGHT OF POLYESTERS 审中-公开
    增加聚酯分子量的方法

    公开(公告)号:WO2012019868A3

    公开(公告)日:2012-04-19

    申请号:PCT/EP2011062189

    申请日:2011-07-18

    Inventor: LOOS ROBERT

    CPC classification number: C08G63/916 C08G81/00

    Abstract: The invention relates to a method for increasing the molecular weight of polyesters by heating 100 parts of polyester with i) 0.01 to 5 parts of a tetracarbolic acid dianhydride, and ii) 0.01 to 5 parts of a copolymer comprising an epoxy group and based on styrene, acrylic acid ester, and/or methacrylic acid ester in an extruder to 160 to 350°C.

    Abstract translation: 本发明涉及一种用于基于苯乙烯,丙烯酸酯增加制备的聚酯的分子量,通过加热100份的聚酯ⅰ)0.01〜5份的四羧酸二酐的和ii)0.01至5重量份的含环氧基的共聚物和/或 甲基丙烯酸酯在160至350℃的挤出机中

    METHOD FOR PRODUCING EXPANDABLE GRANULATES CONTAINING POLYLACTIC ACID
    2.
    发明申请
    METHOD FOR PRODUCING EXPANDABLE GRANULATES CONTAINING POLYLACTIC ACID 审中-公开
    生产可膨胀含聚丙烯酸颗粒的方法

    公开(公告)号:WO2011086030A2

    公开(公告)日:2011-07-21

    申请号:PCT/EP2011050129

    申请日:2011-01-06

    Abstract: The invention relates to a method for producing expandable granulates containing polylactic acid, comprising the following steps: a) melting and mixing the constituents i) between 50 and 99.9 wt. %, relative to the total weight of constituents i) to iii), of polylactic acid, ii) between 0 and 49.9 wt. %, relative to the total weight of constituents i) to iii), of at least one other polymer, iii) between 0.1 and 2 wt. %, relative to the total weight of constituents i) to iii), of a diepoxide or polyepoxide, and iv) between 0 and 10 wt. % of at least one additive, b) mixing v) between 3 and 7 wt. %, relative to the total weight of constituents i) to iv), of an organic blowing agent, into the melted polymer mass, by means of a static or dynamic mixer, at a temperature of at least 40°C, c) discharging the mixture via a nozzle plate with boreholes having a maximum on the nozzle outlet diameter of 1.5 mm, and d) granulating the melted mass containing the blowing agent directly behind the nozzle plate, under water, at a pressure of between 1 and 20 bar. The invention also relates to expandable granulates containing polylactic acid, that can be obtained according to said method, and to special expandable granulates containing polylactic acid, and between 3 and 7 wt. % of an organic blowing agent, preferably n-pentane, and especially preferably iso-pentane. The invention also relates to a preferred method for producing expandable granulates containing polylactic acid and a blowing agent, with a low bulk density.

    Abstract translation: 本发明涉及一种用于制备可膨胀含聚乳酸的颗粒的方法,包括步骤:a)熔化并混合各组分ⅰ)50〜99.9重量%,基于组分的总重量,I至III),聚乳酸二 )0至49.9重量%,基于组分的总重量,i至iii)中,一种或多种其它聚合物,ⅲ)从0.1至2重量%,基于组分的总重量,i至iii)中, 二环氧化物或聚环氧化物和iv)0至10重量%的一种或多种添加剂%,b)将v)的3至7重量%,基于组分的总重量的I至IV)有机发泡剂到聚合物熔体借助于 在至少40℃的温度下的静态或动态混合器,c)通过用造粒孔,其直径在模出口至多1.5毫米,和d)的模板排出吹直接熔融超过管芯板未剂含有 在1到20巴范围内的压力下进行。 此外,本发明涉及通过该方法和特殊可膨胀含聚乳酸的颗粒与3〜7重量的有机发泡剂的重量%,优选正戊烷和更优选异戊烷的比例获得的可膨胀的含聚乳酸的颗粒。 此外,本发明涉及制备具有低堆积密度的含推进剂的可膨胀聚乳酸颗粒的优选方法。

    Método para producir granulados expandibles que contienen poli(ácido láctico)

    公开(公告)号:ES2581309T3

    公开(公告)日:2016-09-05

    申请号:ES13163665

    申请日:2011-01-06

    Applicant: BASF SE

    Abstract: Método para producir granulados expandibles que contienen poli(ácido láctico), el cual comprende las etapas de: a) fundir e incorporar en mezcla los componentes i) 50 a 99,9 % en peso, respecto del peso total de los componentes i a iii, de poli(ácido láctico), ii) 0 a 49,9 % en peso, respecto del peso total de los componentes i a iii, de uno o de varios otros polímeros iii) 0,1 a 2 % en peso, respecto del peso total de los componentes i a iii, de un diepóxido o poliepóxido y iv) 0,1 a 5 % en peso, respecto del peso total de los componentes i y iii, de un agente de nucleación, b) incorporar en mezcla v) 1 a 7 % en peso, respecto del peso total de los componentes i a iv, de un propelente orgánico y vi) 0,01 a 5 % en peso de un co-propelentes, que se selecciona del grupo de nitrógeno, dióxido de carbono, argón, helio o mezclas de los mismos, al polímero fundido por medio de un mezclador estático o dinámico a una temperatura de al menos 140 °C, c) descargar a través de una placa de toberas con perforaciones, cuyo diámetro a la salida de la tobera es de máximo 1,5 mm, y d) granular el material fundido que contiene propelente directamente después de la placa de toberas a una presión en el intervalo de 1 a 20 bar.

    Biodegradable polyester film
    4.
    发明专利

    公开(公告)号:AU2012252446B2

    公开(公告)日:2015-06-25

    申请号:AU2012252446

    申请日:2012-05-09

    Applicant: BASF SE

    Abstract: Biodegradable polyester film comprises: (a) 75-100 wt.% of a biodegradable polyester based on aliphatic and/or aromatic dicarboxylic acids and an aliphatic dihydroxy compound; (b) 0-25 wt.% of polylactic acid; (c) 10-25 wt.% of calcium carbonate; (d) 3-15 wt.% of talc; (e) 0-1 wt.% of an epoxy-containing copolymer based on styrene, acrylic acid esters and/or methacrylic acid ester; and (f) 0-2 wt.% of 2-(4,6-bis-biphenyl-4-yl-1,3,5-triazin-2-yl)-5-(2-ethyl-(n)-hexyloxy)phenol. Independent claims are included for: (1) a master batch containing 75-95 wt.% of the component (a), and the component (b), and 5-25 wt.% of the component (f); and (2) producing mulch film comprising 75-100 wt.% of the component (a), 0-25 wt.% of the component (b), 0-25 wt.% of the component (c), 0-15 wt.% of the component (d), 0-1 wt.% of component (e) and 0.1-1.5 wt.% the component (f).

    BIODEGRADABLE POLYESTER MIXTURE
    5.
    发明专利

    公开(公告)号:CA2891687A1

    公开(公告)日:2014-05-22

    申请号:CA2891687

    申请日:2013-11-08

    Applicant: BASF SE

    Abstract: The invention relates to a biodegradable polyester mixture, containing: i) 45 to 95 wt%, with respect to the total weight of components i and ii, of a polyester I, which is synthesized from: a-1) 40 to 70 wt%, with respect to the total weight of components a and b, of an aliphatic C9-C18 dicarboxylic acid or a C9-C18 dicarboxylic acid derivative; b-1) 30 to 60 wt%, with respect to the total weight of components a and b, of terephthalic acid or a terephthalic acid derivative; c-1) 98 to 100 wt%, with respect to the total weight of components a and b, of a C3-C6 diol; d-1) 0 to 2 wt%, with respect to the total weight of components a and b, of an at least trivalent alcohol; e-1) 0 to 2 wt%, with respect to the total weight of components a to e, of a chain extender; and ii) 5 to 55 wt%, with respect to the total weight of components i and ii, of a polyester II, which is synthesized from: a-2) 40 to 70 wt%, with respect to the total weight of components a and b, of an aliphatic C4-C6 dicarboxylic acid or a C4-C6 dicarboxylic acid derivative; b-2) 30 to 60 wt%, with respect to the total weight of components a and b, of terephthalic acid or a terephthalic acid derivative; c-2) 98 to 100 wt%, with respect to the total weight of components a and b, of a C3-C6 diol; d-2) 0 to 2 wt%, with respect to the total weight of components a and b, of an at least trivalent alcohol; e-2) 0 to 2 wt%, with respect to the total weight of components a to e, of a chain extender. 10 to 25 wt%, with respect to the total weight of polymer mixtures i to iv, of calcium carbonate; and 3 to 15 wt%, with respect to the total weight of polymer mixtures i to iv, of talc.

    BIOLOGISCH ABBAUBARE POLYMERZUSAMMENSETZUNG

    公开(公告)号:DE22204222T1

    公开(公告)日:2025-04-03

    申请号:DE22204222

    申请日:2022-10-27

    Applicant: BASF SE

    Abstract: Biologisch abbaubare Polymerzusammensetzung enthaltenda1) 2 bis 50 Gew.-%, bezogen auf das Gesamtgewicht der Komponenten a1) bis e) der Polymerzusammensetzung, an wenigstens einem Poly(meso-lactid) mit einem anzahlgemittelten Molekulargewicht von wenigstens 20 000 g/mol und einem Verhältnis von L-Milchsäureeinheiten: D-Milchsäureeinheiten von wenigstens 20:80 bis zu 80:20;a2) 0 bis 48 Gew.-%, bezogen auf das Gesamtgewicht der Komponenten a1) bis e), an wenigstens einem Polylactid a2) mit einem Verhältnis von L-Milchsäureeinheiten: D-Milchsäureeinheiten von über 65:35 oder unter35:65, und wobei die Summe von Poly(meso-lactid) a1) und Polylactid a2) höchstens 50 Gew.-%, bezogen auf das Gesamtgewicht der Komponenten a1) bis e), beträgt;b) 20 bis 98 Gew.-%, bezogen auf das Gesamtgewicht der Komponenten a1) bis e) der Polymerzusammensetzung, an wenigstens einem biologisch abbaubaren Polyester ausgewählt aus aliphatischen Polyestern, aliphatisch-aromatischen Polyestern und Copolymeren und Gemischen davon;c) 0 bis 55 Gew.-%, bezogen auf das Gesamtgewicht der Komponenten a1) bis e) der Polymerzusammensetzung, an wenigstens einem Stärkepolymer;d) 0 bis 40 Gew.-%, bezogen auf das Gesamtgewicht der Komponenten a1) bis e) der Polymerzusammensetzung, an wenigstens einem anorganischen Füllstoff; unde) 0 bis 5 Gew.-%, bezogen auf das Gesamtgewicht der Komponenten a1) bis e) der Polymerzusammensetzung, an wenigstens einer Verbindung ausgewählt aus Vernetzern, Gleitmitteln, Kettenverlängerern, Stabilisatoren, Keimbildnern, Gleit- und Trennmitteln, Tensiden, Wachsen, antistatischen Mitteln, Antibeschlagmitteln, Farbstoffen, Pigmenten, UV-Absorbern, UV-Stabilisatoren und andere Kunststoffzusätzen; wobei das anzahlgemittelte Molekulargewicht des Poly(meso-lactids) und das Verhältnis von L-Milchsäureeinheiten: D-Milchsäureeinheiten wie in der Beschreibung beschrieben bestimmt wurden.

    Procedimiento para el revestimiento de papel

    公开(公告)号:ES2398700T3

    公开(公告)日:2013-03-21

    申请号:ES09783286

    申请日:2009-09-22

    Applicant: BASF SE

    Abstract: Procedimiento para el revestimiento de papel, caracterizado porque como agente de revestimiento se emplea unpoliéster biodegradable, alifático-aromático, que contiene: i) un 40 a un 70 % en moles, referido a los componentes i a ii, de uno o varios derivados de ácidodicarboxílico o ácidos dicarboxílicos seleccionados a partir del grupo constituido por: ácido succínico, ácidoadípico, ácido sebácico, ácido azelaico y ácido brasílico; ii) un 60 a un 30 % en moles, referido a los componentes i a ii, de un derivado de ácido tereftálico; iii) un 98 a un 102 % en moles, referido a los componentes i a ii, de un alquilendiol con 2 a 8 átomos decarbono u oxialquilendiol con 2 a 6 átomos de carbono; iv) un 0,00 a un 2 % en peso, referido al peso total de componentes i a iii, de un agente de prolongación decadenas y/o reticulante seleccionado a partir del grupo constituido por: un isocianato di- o polifuncional,isocianurato, oxazolina, epóxido, anhídrido de ácido carboxílico y/o un alcohol al menos trifuncional, o unácido tricarboxílico al menos trifuncional; v) un 0,00 a un 50 % en peso, referido al peso total de componentes i a iv, de una carga orgánicaseleccionada a partir del grupo constituido por: almidón nativo o plastificado, fibras naturales, polvo demadera, y/o de una carga inorgánica seleccionada a partir del grupo constituido por: creta, carbonato decalcio precipitado, grafito, yeso, hollín conductivo, óxido de hierro, cloruro de calcio, dolomita, caolín, dióxidode silicio (cuarzo), carbonato sódico, dióxido de titanio, silicato, volastonita, mica, montmorillonita, talco,fibras de vidrio y fibras minerales, y vi) un 0,00 a un 2 % en peso, referido al peso total de componentes i a iv, de al menos un estabilizador,agente de nucleación, agente deslizante y separador, agente tensioactivo, cera, antiestático, agenteantiempañamiento, colorante, pigmento, filtro UV, estabilizador UV u otro aditivo de material sintético; y con un índice volumétrico de fusión (MVR) según EN ISO 1133 (190ºC, 2,16 kg de peso) de 3 a 50 cm3/10 cm.

Patent Agency Ranking