公开(公告)号:CA2864370A1
公开(公告)日:2013-08-22
申请号:CA2864370
申请日:2013-02-11
Applicant: BASF SE
Inventor: AL-HELLANI RABIE , CIMPEANU CARMEN-ELENA , SCHMIDT-THUMMES JURGEN , LAWRENZ DIRK , GEORGIEVA KRISTINA , SONG ANJA
Abstract: Described is an aqueous polymer dispersion comprising a chain growth addition polymer obtainable via free-radically initiated emulsion polymerization from ethylenically unsaturated, free-radically polymerizable monomers, wherein the chain growth addition polymer is formed to an extent of not less than 60 wt% from primary monomers selected from vinylaromatic compounds, conjugated aliphatic dienes, vinyl esters of saturated C1- to C20-carboxylic acids, esters of acrylic acid or of methacrylic acid with monohydric C1- to C20-alcohols, aliphatic hydrocarbons having 2 to 8 carbon atoms and one or two double bonds, or mixtures thereof, wherein the monomers are polymerized in the presence of lignosulfonate and wherein the chain growth addition polymer is branched or crosslinked. Also described is a process for preparing the aqueous polymer dispersion. The polymer dispersion is useful for preparing paper coating compositions.
-
公开(公告)号:CA2700059C
公开(公告)日:2015-01-20
申请号:CA2700059
申请日:2008-10-06
Applicant: BASF SE
Inventor: EVSTATIEVA ELITSA , SCHMIDT-THUMMES JURGEN , LAWRENZ DIRK , MINDERHOUD JOHANNES JAN-BESSEL , ARENS GUILLERMO
IPC: C08F251/02 , C08F2/22 , C08L25/10 , C08L51/02 , C09D151/02 , D21H19/54 , D21H19/58 , D21H21/16
Abstract: Aqueous polymer dispersions based on copolymers formed from vinyl-aromatics and conjugated aliphatic dienes having a mean particle size of from 80 to 150 nm are obtainable by free-radically initiated emulsion copolymerization of (a) from 19.9 to 80 parts by weight of at least one vinylaromatic compound, (b) from 19.9 to 80 parts by weight of at least one conjugated aliphatic diene, (c) from 0.1 to 10 parts by weight of at least one ethylenically unsaturated acid and (d) from 0 to 20 parts by weight of at least one other monoethylenically unsaturated monomer, where the sum of the parts by weight of monomers (a), (b), (c) and (d) is always 100, in an aqueous medium in the presence of at least one degraded starch with an intrinsic viscosity .eta. of less than 0.07 dl/g, using at least 0.9% by weight, based on all of the monomers used, of initiators selected from peroxodisulphates, peroxosulphates, azo initiators, organic peroxides, organic hydroperoxides and hydrogen peroxide, wherein at least 30% by weight of the initiators are initially charged in the aqueous medium together with the degraded starch and the monomers and the remaining initiators are metered into this initial charge under polymerization conditions. Processes for preparing this dispersion by emulsion polymerization of the monomers (a), (b), (c) and optionally (d) in the presence of a degraded starch with an intrinsic viscosity .eta. of less than 0.07 dl/g, where a portion of the initiator is initially charged together with the aqueous solution of the degraded starch in the reactor, and the remaining initiator and the monomers are metered in under polymerization conditions, and the use of the aqueous polymer dispersions as binders, adhesives, sizes for fibres or for producing coatings.
-
公开(公告)号:AU2011267134A1
公开(公告)日:2013-01-10
申请号:AU2011267134
申请日:2011-06-14
Applicant: BASF SE
Inventor: SCHMIDT-THUMMES JURGEN , EVSTATIEVA ELITSA , MOREL AURELIE , LAWRENZ DIRK , SEYFFER HERMANN
IPC: C08F220/18 , C08F2/22 , C08F212/08 , D21H19/58
Abstract: Aqueous polymer dispersions and processes for preparing them are described. The polymer dispersions can be obtained by free-radically initiated emulsion polymerization of from 19.9 to 80 parts by weight of vinylaromatic compounds, from 19.9 to 80 parts by weight of acrylate monomers selected from among C1‑C10-alkyl acrylates and C1-C10-alkyl methacrylates, from 0.1 to 10 parts by weight of ethylenically unsaturated acids and from 0 to 20 parts by weight of other ethylenically unsaturated monomers, wherein the emulsion polymerization is carried out in an aqueous medium in the presence of free-radical-forming initiators, seed latex and at least one carbohydrate compound in the form of a degraded starch. The polymer dispersions are particularly suitable for producing paper coating compositions.
-
-
公开(公告)号:AU2009319065A1
公开(公告)日:2010-06-03
申请号:AU2009319065
申请日:2009-11-20
Applicant: BASF SE
Inventor: EVSTATIEVA ELITSA , SCHMIDT-THUMMES JURGEN , LAWRENZ DIRK
IPC: C08F251/00 , C08B31/00 , C08F251/02 , C08F279/02 , C08F279/04 , C08L51/02 , C08L55/02 , C09D151/02 , C09D155/02 , D21H19/54 , D21H19/58
-
公开(公告)号:ZA201104644B
公开(公告)日:2012-09-26
申请号:ZA201104644
申请日:2011-06-23
Applicant: BASF SE
Inventor: EVSTATIEVA ELITSA , SCHMIDT-THUMMES JURGEN , LAWRENZ DIRK
IPC: C08F20060101 , C08B20060101 , C08L20060101 , C09D20060101 , D21H20060101
-
公开(公告)号:ES2163211T5
公开(公告)日:2009-10-16
申请号:ES97953687
申请日:1997-11-21
Applicant: BASF SE
Inventor: KELLER ANDREAS , LAWRENZ SVEN , BAUER GERHARD , SCHMIDT-THUMMES JURGEN , BACHER REINHARD , HARTMANN JURGEN
Abstract: LA PRESENTE INVENCION TRATA DE UN PROCEDIMIENTO PARA LA PREPARACION DE UNA DISPERSION POLIMERICA MEDIANTE LA POLIMERIZACION RADICAL DE UNA EMULSION ACUOSA DE MONOMEROS, QUE SE CARACTERIZA PORQUE LA EMULSION DE MONOMEROS SE PREPARA DE MANERA CONTINUA EN FUNCION DEL GASTO.
-
公开(公告)号:CA2700059A1
公开(公告)日:2009-04-16
申请号:CA2700059
申请日:2008-10-06
Applicant: BASF SE
Inventor: EVSTATIEVA ELITSA , SCHMIDT-THUMMES JURGEN , LAWRENZ DIRK , MINDERHOUD JOHANNES JAN-BESSEL , ARENS GUILLERMO
IPC: C08F251/02 , C08F2/22 , C08L25/10 , C08L51/02 , C09D151/02 , D21H19/54 , D21H19/58 , D21H21/16
Abstract: Aqueous polymer dispersions based on copolymers formed from vinyl-aromatics and conjugated aliphatic dienes having a mean particle size of from 80 to 150 nm are obtainable by free-radically initiated emulsion copolymerization of (a) from 19.9 to 80 parts by weight of at least one vinylaromatic compound, (b) from 19.9 to 80 parts by weight of at least one conjugated aliphatic diene, (c) from 0.1 to 10 parts by weight of at least one ethylenically unsaturated acid and (d) from 0 to 20 parts by weight of at least one other monoethylenically unsaturated monomer, where the sum of the parts by weight of monomers (a), (b), (c) and (d) is always 100, in an aqueous medium in the presence of at least one degraded starch with an intrinsic viscosity ? of less than 0.07 dl/g, using at least 0.9% by weight, based on all of the monomers used, of initiators selected from peroxodisulphates, peroxosulphates, azo initiators, organic peroxides, organic hydroperoxides and hydrogen peroxide, wherein at least 30% by weight of the initiators are initially charged in the aqueous medium together with the degraded starch and the monomers and the remaining initiators are metered into this initial charge under polymerization conditions. Processes for preparing this dispersion by emulsion polymerization of the monomers (a), (b), (c) and optionally (d) in the presence of a degraded starch with an intrinsic viscosity ? of less than 0.07 dl/g, where a portion of the initiator is initially charged together with the aqueous solution of the degraded starch in the reactor, and the remaining initiator and the monomers are metered in under polymerization conditions, and the use of the aqueous polymer dispersions as binders, adhesives, sizes for fibres or for producing coatings.
-
公开(公告)号:AU2011267134B2
公开(公告)日:2015-02-26
申请号:AU2011267134
申请日:2011-06-14
Applicant: BASF SE
Inventor: SCHMIDT-THUMMES JURGEN , EVSTATIEVA ELITSA , MOREL AURELIE , LAWRENZ DIRK , SEYFFER HERMANN
IPC: C08F220/18 , C08F2/22 , C08F212/08 , D21H19/58
Abstract: Aqueous polymer dispersions and processes for preparing them are described. The polymer dispersions can be obtained by free-radically initiated emulsion polymerization of from 19.9 to 80 parts by weight of vinylaromatic compounds, from 19.9 to 80 parts by weight of acrylate monomers selected from among C1‑C10-alkyl acrylates and C1-C10-alkyl methacrylates, from 0.1 to 10 parts by weight of ethylenically unsaturated acids and from 0 to 20 parts by weight of other ethylenically unsaturated monomers, wherein the emulsion polymerization is carried out in an aqueous medium in the presence of free-radical-forming initiators, seed latex and at least one carbohydrate compound in the form of a degraded starch. The polymer dispersions are particularly suitable for producing paper coating compositions.
-
10.
公开(公告)号:CA2854354A1
公开(公告)日:2013-05-02
申请号:CA2854354
申请日:2012-10-26
Applicant: BASF SE
Inventor: LAWRENZ DIRK , SCHMIDT-THUMMES JURGEN , VELING NICO
Abstract: Paper coating compositions comprise inorganic pigments and an aqueous polymeric dispersion comprising dispersed polymeric particles. The polymers are obtainable by polymerization of a first monomer that is liquid at room temperature, has a boiling point of at least 50°C and a glass transition temperature of at least 20°C as homopolymer, and a second monomer that is gaseous at room temperature, has a boiling point of below 0°C and a glass transition temperature of below -30°C as homopolymer. The dispersed polymeric particles have an average size of below 150 nm and a glass transition temperature in the range from -10 to +30°C.
-
-
-
-
-
-
-
-
-