1.
    发明专利
    未知

    公开(公告)号:DE69006353T2

    公开(公告)日:1994-06-23

    申请号:DE69006353

    申请日:1990-05-25

    Applicant: IBM

    Abstract: A method for cleaving semiconductor wafers, or segments thereof, which comprises placing the wafer (11), provided with scribe lines (15) defining the planes where cleaving is to take place, inbetween a pair of flexible transport bands (12,13) and guiding it around a curved, large radius surface (21) thereby applying a bending moment. With a moment of sufficient magnitude, individual bars (22) are broken off the wafer as this is advanced, the bars having front- and rear-end facets. On cleaving, each bar, while still pressed against the curved surface, is automatically separated whereby mutual damage of the facets of neighbouring bars is prevented. For further handling, e.g. for the transport of the bars to an evaporation station for passivation layer deposition, provisions are made to keep the bars separated. Cleaving and the subsequent passivation coating can be carried out in-situ in a vacuum system to prevent facet contamination prior to applying the passivation.

    2.
    发明专利
    未知

    公开(公告)号:DE69006353D1

    公开(公告)日:1994-03-10

    申请号:DE69006353

    申请日:1990-05-25

    Applicant: IBM

    Abstract: A method for cleaving semiconductor wafers, or segments thereof, which comprises placing the wafer (11), provided with scribe lines (15) defining the planes where cleaving is to take place, inbetween a pair of flexible transport bands (12,13) and guiding it around a curved, large radius surface (21) thereby applying a bending moment. With a moment of sufficient magnitude, individual bars (22) are broken off the wafer as this is advanced, the bars having front- and rear-end facets. On cleaving, each bar, while still pressed against the curved surface, is automatically separated whereby mutual damage of the facets of neighbouring bars is prevented. For further handling, e.g. for the transport of the bars to an evaporation station for passivation layer deposition, provisions are made to keep the bars separated. Cleaving and the subsequent passivation coating can be carried out in-situ in a vacuum system to prevent facet contamination prior to applying the passivation.

Patent Agency Ranking