12.
    发明专利
    未知

    公开(公告)号:DE10336452A1

    公开(公告)日:2005-03-03

    申请号:DE10336452

    申请日:2003-08-06

    Applicant: BASF AG

    Abstract: An epichlorohydrinamine polymer has a ratio of amine units to epichlorohydrin units of from 0.8:1.2 to 1.0:1.0, dimethylaminopropylamine and benzylamine preferably being used as amine and/or ammonium units. The novel epichlorohydrinamine polymer is used, for example, for the surface treatment of semifinished leather products and textile materials.

    13.
    发明专利
    未知

    公开(公告)号:DE59711218D1

    公开(公告)日:2004-02-19

    申请号:DE59711218

    申请日:1997-10-17

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP97/05744 Sec. 371 Date May 12, 1999 Sec. 102(e) Date May 12, 1999 PCT Filed Oct. 17, 1997 PCT Pub. No. WO98/17764 PCT Pub. Date Apr. 30, 1998The invention relates to the use of crosslinked nitrogenous compounds which are soluble or dispersible in water and are obtainable by crosslinking of (a) compounds containing at least three NH groups with (b) at least bifunctional crosslinkers which react with NH groups, in detergents and cleaners, especially soil release agents. Compounds (a) are preferably selected from the group consisting of oligo- and polyamines, polyalkylenepolyamines, polyamidoamines, polyamidoamines grafted with (poly)ethyleneimnine, and mixtures thereof

    15.
    发明专利
    未知

    公开(公告)号:BRPI0413268A

    公开(公告)日:2006-10-10

    申请号:BRPI0413268

    申请日:2004-08-06

    Applicant: BASF AG

    Abstract: An epichlorohydrinamine polymer has a ratio of amine units to epichlorohydrin units of from 0.8:1.2 to 1.0:1.0, dimethylaminopropylamine and benzylamine preferably being used as amine and/or ammonium units. The novel epichlorohydrinamine polymer is used, for example, for the surface treatment of semifinished leather products and textile materials.

    20.
    发明专利
    未知

    公开(公告)号:DE19908462A1

    公开(公告)日:2000-08-31

    申请号:DE19908462

    申请日:1999-02-26

    Applicant: BASF AG

    Abstract: The invention relates to a method for the hydroformylation of olefins with at least 7 carbon atoms. According to said method a) the olefin is subjected to a hydroformylation reaction together with carbon monoxide and hydrogen in the presence of a complex consisting of rhodium and a polymeric complex ligand with more than 10 nitrogen atoms and having a molar mass greater than 1000 g/ mol, as well as a solubilizing agent, at a temperature of between 40 and 200 DEG C and a pressure of between 1 and 600 bar in a reaction zone, such that in these reaction conditions the solubilizing agent together with the olefin and the resulting hydroformylation product forms a largely uniform phase in which the complex is solubilized; b) in said reaction mixture a phase separation into a phase rich in solubilizing agent and a phase poor in solubilizing agent is induced, the complex preferably being present in the phase rich in solubilizing agent and the hydroformylation product preferably present in the phase poor in solubilizing agent; and c) the above phases are separated. Phase separation is preferably induced by cooling or by addition of a phase-separating agent such as water.