Abstract:
adding an organic solvent to the stainless steel scrap generated in surface grinding process of the stainless steel; dissolving the degreased scrap in strong acid and filtering it to add alkali; granulating the filtered scrap in polymeric granulating agent and sieving it; and reducing the sieved stainless steel powder at 900-1200 deg.C for 1-3 hrs. under H2 gas atmosphere.
Abstract:
The waterproof gypsum-foam body is manufactured by mixing burnt gypsum with 0.5-10 wt.% waterproofing agent and 0.5-10 wt.% calcium hydroxide to the dry powdered gypsum, mixing the mixt. with the foam made of water and foaming-agent, pouring it in a mould, drying at room temp., and demoulding. The foaming agent is polyvinyl alcohol, surfactant or their admixture and the waterproofing agent is the dry mixture powder of aqueous silicon resin and burnt gypsum.
Abstract:
A waterproof foamed gypsum is produced by mxing lime slurry, accelator and polyvinyl alcohol foams, and slip casting. The line slurry comprises 100 wt.% burnt plaster, 0.5 wt.% aq. silicon resin, 10 wt.% calcium hydroxide and a little retarder. The producted gypsum has a good waterproofing, fireproofing, sound proofing and insulating property.
Abstract:
The present invention relates to a method for continuously producing a group iii nitride crystal powder, which reduces the process of connection and transport of a reactor over an existing ammonothermal synthesis reaction; minimizes contamination from oxygen and moisture by blocking the reactor from external air; and reduces the processing hours, thereby providing a reactor with excellent productivity for ammonothermal synthesis, by continuously pouring raw materials while maintaining a constant temperature and continuously collecting the powder whose reaction is finished.
Abstract:
PURPOSE: An europium oxynitride phosphor is provided to selectively use the phosphor, and to prevent the reduction of the brightness of the phosphor when being exposed to air or an excitation source. CONSTITUTION: An europium oxynitride phosphor irradiates lights by activating a mother body marked with chemical formula 1: (Eu_(1-a-b-d)A_aB_bD_d)E_eO_xN_z. In the chemical formula 1, A is one or two elements selected from the group consisting of Lanthanum group metal elements. B is one or two elements selected from the group consisting of divalent metal elements. D is one or two elements selected from the group consisting of trivalent metal elements. E is one or two elements selected from the group consisting of tetravalent metal elements.