公开(公告)号:DE59307290D1
公开(公告)日:1997-10-16
申请号:DE59307290
申请日:1993-01-28
Applicant: BASF AG
Inventor: JAEGER ULRICH DR , BECK ERICH DR , REICH WOLFGANG DR , BRONSTERT BERND DR , HUEMMER WOLFGANG DR
IPC: C08F299/06 , C08G18/08 , C08G18/38 , C08G18/67 , C08G18/78 , C08G18/79 , C08J3/03 , C09D175/14
-
公开(公告)号:DE19539533A1
公开(公告)日:1997-04-30
申请号:DE19539533
申请日:1995-10-24
Applicant: BASF AG
Inventor: BECHTEL SIEGFRIED , ULONSKA ARMIN DR , HEILIG EDWIN , REICH WOLFGANG DR
-
公开(公告)号:DE4445853A1
公开(公告)日:1996-06-27
申请号:DE4445853
申请日:1994-12-22
Applicant: BASF AG
IPC: C08F8/00 , C08K5/103 , C08L23/14 , C08F255/02
Abstract: Partly crosslinked plastic materials (A) with a melt flow index 230/2.16 of 0.1-100 g/10 minutes are obtd from: (a1) a polymer contg: (a1.1) 25-97 wt% of a copolymer of propylene with 0.1-15 wt% 2-10C alkene-1, and (a1.2) 3-75 wt% of a copolymer of propylene with 15-80 wt% 2-10C alkene-1; or (a2) a polymer contg: (a2.1) 25-97 wt% propylene homopolymer, and (a2.2) 3-75 wt% copolymer (a1.2) as above; or (a3) a propylene homopolymer with a melt flow index 230/2 of 0.1-100 g/10 minutes; or (a4) a statistical propylene copolymer contg less than 15 wt% 2-10C alkene-1 comonomer; and (b) a cpd of formula: (H2C=CR-COO)nX (I) R = H or 1-4C alkyl; X = 1-30C alkyl or 7-30C aralkyl, opt contg in-chain O and/or N atom(s); and n = 2 or 3; and these materials (A) are obtd by reacting (a1), (a2), (a3) or (a4) with cpd (b) at 180-280 deg C and 1-100 bar for a mean residence time of 0.2-10 minutes. Also claimed are: (i) a process for the prodn of (A) by reacting the above polymers with (b) at 190-260 deg C and 1-60 bar for a mean residence time of 0.2-5 minutes, pref immediately after prodn of the polymer in a mixer connected to the polymerisation reactor; and (ii) films, fibres and mouldings made from (A).
-
公开(公告)号:ES2083887T3
公开(公告)日:1996-04-16
申请号:ES94116764
申请日:1994-10-25
Applicant: BASF AG
Inventor: KEMPTER FRITZ ERDMANN DR , REICH WOLFGANG DR , HOFMANN JURGEN
IPC: C08F2/02 , C08F2/06 , C08F8/14 , C08F8/00 , C08F20/10 , C08F220/14 , C08F290/00 , C08F299/00 , C09D4/06 , C09D5/03 , C09D133/04
Abstract: A process for the preparation of free-radical-crosslinkable copolymers by polymer-analogous reaction of A) a copolymer (A) comprising a1) from 20 to 85 mol % of a monomer (a1) containing the methacrylic acid structural unit and a2) from 15 to 80 mol % of another free-radical-polymerising monomer (a2), where a3) from 5 to 50 mol % of the total amount of the monomers (a1) and (a2) are monomers (a3) carrying functional groups which are capable of a condensation or addition reaction, with B) an olefinically unsaturated monomer (B) carrying a functional group which is complementary to that of the monomers (a3), characterised in that the polymer-analogous reaction is carried out at from 90 to 150 DEG C and at a mean residence time of from 3 to 20 minutes in highly concentrated solution or in bulk. The free-radical-crosslinkable copolymers which can be prepared by this process are used as binders for powder coatings (paints).
-
公开(公告)号:DE59400150D1
公开(公告)日:1996-04-11
申请号:DE59400150
申请日:1994-10-25
Applicant: BASF AG
Inventor: KEMPTER FRITZ ERDMANN DR , REICH WOLFGANG DR , HOFMANN JUERGEN
IPC: C08F8/00 , C08F2/02 , C08F2/06 , C08F8/14 , C08F20/10 , C08F220/14 , C08F290/00 , C08F299/00 , C09D4/06 , C09D5/03 , C09D133/04
Abstract: A process for the preparation of free-radical-crosslinkable copolymers by polymer-analogous reaction of A) a copolymer (A) comprising a1) from 20 to 85 mol % of a monomer (a1) containing the methacrylic acid structural unit and a2) from 15 to 80 mol % of another free-radical-polymerising monomer (a2), where a3) from 5 to 50 mol % of the total amount of the monomers (a1) and (a2) are monomers (a3) carrying functional groups which are capable of a condensation or addition reaction, with B) an olefinically unsaturated monomer (B) carrying a functional group which is complementary to that of the monomers (a3), characterised in that the polymer-analogous reaction is carried out at from 90 to 150 DEG C and at a mean residence time of from 3 to 20 minutes in highly concentrated solution or in bulk. The free-radical-crosslinkable copolymers which can be prepared by this process are used as binders for powder coatings (paints).
-
公开(公告)号:DE4337482A1
公开(公告)日:1995-05-04
申请号:DE4337482
申请日:1993-11-03
Applicant: BASF AG
Inventor: KEMPTER FRITZ ERDMANN DR , REICH WOLFGANG DR , HOFMANN JUERGEN
IPC: C08F8/00 , C08F2/02 , C08F2/06 , C08F8/14 , C08F20/10 , C08F220/14 , C08F290/00 , C08F299/00 , C09D4/06 , C09D5/03 , C09D133/04 , C08F220/00 , C08J3/24 , C08J3/28 , B05D3/06 , B29B7/42
Abstract: A process for the preparation of free-radical-crosslinkable copolymers by polymer-analogous reaction of A) a copolymer (A) comprising a1) from 20 to 85 mol % of a monomer (a1) containing the methacrylic acid structural unit and a2) from 15 to 80 mol % of another free-radical-polymerising monomer (a2), where a3) from 5 to 50 mol % of the total amount of the monomers (a1) and (a2) are monomers (a3) carrying functional groups which are capable of a condensation or addition reaction, with B) an olefinically unsaturated monomer (B) carrying a functional group which is complementary to that of the monomers (a3), characterised in that the polymer-analogous reaction is carried out at from 90 to 150 DEG C and at a mean residence time of from 3 to 20 minutes in highly concentrated solution or in bulk. The free-radical-crosslinkable copolymers which can be prepared by this process are used as binders for powder coatings (paints).
-
公开(公告)号:ES2083887T5
公开(公告)日:1999-11-01
申请号:ES94116764
申请日:1994-10-25
Applicant: BASF AG
Inventor: KEMPTER FRITZ ERDMANN DR , REICH WOLFGANG DR , HOFMANN JURGEN
IPC: C08F2/02 , C08F2/06 , C08F8/14 , C08F8/00 , C08F20/10 , C08F220/14 , C08F290/00 , C08F299/00 , C09D4/06 , C09D5/03 , C09D133/04
Abstract: A process for the preparation of free-radical-crosslinkable copolymers by polymer-analogous reaction of A) a copolymer (A) comprising a1) from 20 to 85 mol % of a monomer (a1) containing the methacrylic acid structural unit and a2) from 15 to 80 mol % of another free-radical-polymerising monomer (a2), where a3) from 5 to 50 mol % of the total amount of the monomers (a1) and (a2) are monomers (a3) carrying functional groups which are capable of a condensation or addition reaction, with B) an olefinically unsaturated monomer (B) carrying a functional group which is complementary to that of the monomers (a3), characterised in that the polymer-analogous reaction is carried out at from 90 to 150 DEG C and at a mean residence time of from 3 to 20 minutes in highly concentrated solution or in bulk. The free-radical-crosslinkable copolymers which can be prepared by this process are used as binders for powder coatings (paints).
-
公开(公告)号:DE19753322A1
公开(公告)日:1999-06-10
申请号:DE19753322
申请日:1997-12-02
Applicant: BASF AG
Inventor: KOENIGER RAINER DR , PAULUS WOLFGANG DR , REICH WOLFGANG DR , BECK ERICH DR , WOLF LOTHAR
IPC: C07C67/08 , C07C67/26 , C07C69/54 , C08F2/42 , C08F2/46 , C08F20/18 , C08F20/32 , C08F299/02 , C08G59/17 , C08L63/10 , C09D4/02 , C09D4/06 , C09D163/10 , C08L33/14 , C08L33/08 , C08L33/10 , C08J3/28
Abstract: A mixture (I) of acrylic or methacrylic compounds contains 40-95 wt.% epoxy (meth)acrylate and is prepared by: (a) esterification of hydroxyl compounds with acrylic acid or methacrylic acid; (b) optionally addition of further acrylic acid or methacrylic acid and (c) reaction of the excess acrylic or methacrylic acid with epoxide in the presence of the ester product from (a). Independent claims are included for: (i) a radiation curable composition (II) containing (I); and (ii) a process for the curing of (II) by subjecting (II) to energy intensive light or electron beams.
-
公开(公告)号:DE19732621A1
公开(公告)日:1999-02-04
申请号:DE19732621
申请日:1997-07-29
Applicant: BASF AG
Inventor: SCHWARTZ MANFRED DR , MENZEL KLAUS , BECHERT BERTOLD , BECK ERICH DR , REICH WOLFGANG DR
IPC: C04B41/48 , C04B41/52 , C04B41/63 , C04B41/70 , C08F2/46 , C09D175/16 , C09D183/07 , B05D7/24 , C08F220/18 , C09D167/07 , C09D171/02 , C09D163/10 , C09D161/28 , C09D133/04
Abstract: The use of radiation-curable preparations contains polymer(s) P1 with ethylenic double bonds for coating moulded products containing mineral binders (mineral mouldings). Also claimed is (i) a process for the production of coated mineral mouldings by applying this type of preparation to the surface of a moulded product, possibly removing any solvent, and hardening with UV or electron beam radiation; (ii) coated mineral mouldings obtained by this process.
-
公开(公告)号:DE19716020A1
公开(公告)日:1998-10-22
申请号:DE19716020
申请日:1997-04-17
Applicant: BASF AG
Inventor: KOKEL NICOLAS DR , MENZEL KLAUS DIPL ING , REICH WOLFGANG DR
IPC: C09D175/04 , C09D175/16 , C08J3/03 , C08L75/04 , D06N3/00 , C08G18/40 , C08G18/65 , C08G18/34 , C08G18/38 , C08G18/10 , C08G18/67
Abstract: The present invention describes aqueous dispersions which are substantially free of protective colloids or emulsifiers, containing in a dispersed form a) a polyurethane (A) containing hydrophilic groups, causing water dispersion of said polyurethane which is substantially free of C-C double bonds and b) a prepolymer containing 0.1 to 1 mol radically polymerizable C-C double bonds per 100 gr. of prepolymer.
-
-
-
-
-
-
-
-
-