51.
公开(公告)号:CA2575008A1
公开(公告)日:2006-03-02
申请号:CA2575008
申请日:2005-08-04
Applicant: BASF AG
Inventor: GOETHLICH ALEXANDER , WITTELER HELMUT , DIETSCHE FRANK , KLUEGLEIN MATTHIAS , KLIPPEL FRANK , SCHORNICK GUNNAR
IPC: C23C22/53 , C09D5/08 , C23C22/56 , C23F11/173
Abstract: A process for passivating a metallic surface by treating it with an acidic aqueous preparation comprising at least one itaconic acid homo- or copolymer. Passivating layers and metallic surfaces obtainable by means of the process.
-
公开(公告)号:PT1074570E
公开(公告)日:2004-09-30
申请号:PT00122950
申请日:1995-06-27
Applicant: BASF AG
Inventor: SCHORNICK GUNNAR , WARZELHAN VOLKER , SEELIGER URSULA , YAMAMOTO MOTONORI , BAUER PETER , BRUCHMANN BERND
IPC: A01G13/02 , C08G18/42 , C08G18/46 , C08L3/00 , C08G18/66 , C08G63/00 , C08G63/183 , C08G63/20 , C08G63/60 , C08G63/688 , C08G63/91 , C08L3/02 , C08L67/02 , C08L75/06 , C08L101/16 , C09D167/00 , C09K17/52
Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd
-
公开(公告)号:DE10312509A1
公开(公告)日:2004-09-30
申请号:DE10312509
申请日:2003-03-20
Applicant: BASF AG
Inventor: LEYRER REINHOLD J , MUELLER BETTINA , AMRHEIN PATRICK , SCHORNICK GUNNAR , RITTER HELMUT
Abstract: A process for preparing a polymer having isotactic or syndiotactic regions (ordered regions for short) by polymerizing polymerizable compounds (monomers) in the presence of an optically active compound as complexing agent, wherein more than 50% by weight of the optically active compound is in the form of only one of the possible enantiomers, the polymerization takes place at temperatures below 20° C., and at least 10% by weight of the monomers are prochiral compounds.
-
公开(公告)号:AT265485T
公开(公告)日:2004-05-15
申请号:AT00122950
申请日:1995-06-27
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , SCHORNICK GUNNAR , BRUCHMANN BERND , SEELIGER URSULA , YAMAMOTO MOTONORI , BAUER PETER
IPC: C08L3/00 , A01G13/02 , C08G18/42 , C08G18/46 , C08G18/66 , C08G63/00 , C08G63/183 , C08G63/20 , C08G63/60 , C08G63/688 , C08G63/91 , C08L3/02 , C08L67/02 , C08L75/06 , C08L101/16 , C09D167/00 , C09K17/52
Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd
-
公开(公告)号:ES2201281T3
公开(公告)日:2004-03-16
申请号:ES97914304
申请日:1997-03-25
Applicant: BASF AG
Inventor: BAUR RICHARD , BERTLEFF WERNER , POTTHOFF-KARL BIRGIT , EHLE BEATE , KRONER MATTHIAS , SCHORNICK GUNNAR
IPC: C11D3/30 , C11D1/40 , C11D1/83 , C11D3/00 , C11D3/08 , C11D3/10 , C11D3/36 , C11D3/37 , C11D3/39 , C11D7/08 , C11D7/32
Abstract: A mixture comprising(a) from 0.1 to 99% by weight of at least one polycarboxylate having at least 3 carboxyls,(b) from 0.1 to 99% by weight of at least one amine having a pKa value of more than 9, and(c) from 0.1 to 99% by weight of at least one acid selected from the group consisting of mineral acids and organic acids having one or two carboxyls and not more than 10 carbons,with the proviso that the mixture contains less than 24% by weight of triphosphates, is used in detergent and rinse aid formulations.
-
公开(公告)号:ES2190948T3
公开(公告)日:2003-09-01
申请号:ES00907592
申请日:2000-02-21
Applicant: BASF AG
Inventor: HAHNLE HANS-JOACHIM , SCHRODER ULRICH , HEIDER WOLFGANG , SCHORNICK GUNNAR , ANSTOCK THOMAS
Abstract: Water-absorbing, expanded, crosslinked polymers obtainable by(I) foaming a polymerizable aqueous mixture which comprises(a) monoethylenically unsaturated monomers which contain acidic groups and are optionally neutralized,(b) optionally other monoethylenically unsaturated monomers,(c) crosslinkers,(d) initiators,(e) 0.1-20% by weight of at least one surfactant,(f) optionally at least one solubilizer and(g) optionally thickeners, foam stabilizers, polymerization regulators, fillers and/or cell nucleating agents,where the foaming takes place by dissolving a gas which is inert to free radicals under a pressure of 2-400 bar in the polymerizable aqueous mixture, and then decompressing the latter to atmospheric pressure, and(II) polymerizing the foamed mixture to form an expanded hydrogel and, where appropriate, adjusting the water content of the expanded polymer to 1-60% by weight, process for preparing the water-absorbing, expanded, crosslinked polymers and use of these polymers in sanitary articles employed for absorbing body fluids, in dressing material for covering wounds, as sealing material, as soil improver, as soil substitute and as packaging material.
-
公开(公告)号:ES2183878T3
公开(公告)日:2003-04-01
申请号:ES95924943
申请日:1995-06-27
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , SCHORNICK GUNNAR , BRUCHMANN BERND , SEELIGER URSULA , YAMAMOTO MOTONORI , BAUER PETER
IPC: C08L3/00 , A01G13/02 , C08G18/42 , C08G18/46 , C08G18/66 , C08G63/00 , C08G63/183 , C08G63/20 , C08G63/60 , C08G63/688 , C08G63/91 , C08L3/02 , C08L67/02 , C08L75/06 , C08L101/16 , C09D167/00 , C09K17/52
Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd
-
公开(公告)号:DE10055084A1
公开(公告)日:2002-06-13
申请号:DE10055084
申请日:2000-11-07
Applicant: BASF AG
Inventor: DIETZEN FRANZ-JOSEF , HAEHNLE HANS-JOACHIM , EVSIOUKOV SERGUEI , SCHORNICK GUNNAR , EHRMANN GERD , FUNK RUEDIGER
IPC: C08J9/12 , A61F13/15 , A61L15/42 , B29C47/00 , B29K23/00 , B29K67/00 , B29K105/04 , C08J9/14 , C08J9/36 , C08J9/04 , C08J9/228 , C08J7/12 , B29C44/50
Abstract: Flexible foams based on olefin polymers or thermoplastic polyesters comprise more than 40% open cells and have a density of less than 300 g/l and an average cell diameter of less than 0.1 mm. Independent claims are also included for: (1) a process for producing the foams, comprising extruding a polymer melt together with 2-40 wt.% of a strongly nucleating liquid propellant; and (2) use of flexible, open-celled, microcellular extruder foams based on thermoplastic polymers to produce liquid-absorbing hygiene articles. 24
-
公开(公告)号:NO311032B1
公开(公告)日:2001-10-01
申请号:NO973228
申请日:1997-07-11
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , SCHORNICK GUNNAR , BAUMANN EDWIN , SEELIGER URSULA , YAMAMOTO MOTONORI , RAMLOW GERHARD
IPC: C08G18/60 , C08G69/44 , C08G73/04 , C08J9/04 , C08L1/02 , C08L77/12 , C08L101/16 , C09D175/12 , C09J177/12 , D21H19/30
Abstract: Biodegradable polyesteramides as defined in the specification are obtained by reacting a mixture consisting essentially ofa1) a mixture consisting essentially of35 to 95 mol % of adipic acid or ester-forming derivatives thereof,5 to 65 mol % of terephthalic acid or ester-forming derivatives thereof, and0 to 5 mol % of a compound containing sulfonate groups,a2) a mixture consisting essentially of95.5 to 0.5 mol % of a dihydroxy compound,0.5 to 99.5 mol % of an amino-C2-C12-alkanol or an amino-C5-C10-cycloalkanol,0 to 50 mol % of a diamino-C1-C8-alkane, and0 to 50 mol % of a 2,2'-bisoxazoline of the formula I wherein R1 is as set forth in the specification, anda3) 0 to 5 mol %, based on a1), of a compound D as set forth in the specification;and other biodegradable polymers and thermoplastic molding compositions, their manufacture and their use for producing biodegradable moldings, adhesives, foams, and coatings.
-
60.
公开(公告)号:NZ289416A
公开(公告)日:2000-01-28
申请号:NZ28941695
申请日:1995-06-27
Applicant: BASF AG
Inventor: WARZELHAN VOLKER , SCHORNICK GUNNAR , BRUCHMANN BERND , SEELIGER URSULA , YAMAMOTO MOTONORI , BAUER PETER
IPC: A01G13/02 , C08G18/42 , C08G18/46 , C08L3/00 , C08G18/66 , C08G63/00 , C08G63/183 , C08G63/20 , C08G63/60 , C08G63/688 , C08G63/91 , C08L3/02 , C08L67/02 , C08L75/06 , C08L101/16 , C09D167/00 , C09K17/52
Abstract: iodegradable polyesters P1 obtainable by the reaction of a mixture consisting essentially of (a1) a mixture essentially of 35 to 95 mol% adipic acid or ester-forming derivatives thereof or mixtures thereof, 5 to 65 mol% terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0 to 5 mol% of a sulphonate group-containing compound in which the sum of the individual mol percentages is 100, and (a2) a dihydroxy compound selected from the group consisting of C2-C6 alkane diols and C5-C10 cycloalkane diols, in which the molar ratio of (a1) and (a2) is in the range from 0.4:1 to 1.5:1, provided that the polyester P1 have a molecular weight (Mn) in the range from 5000 to 50,000 g/mol, a viscosity index in the range from 30 to 350 g/ml (measured in o-dichlorobenzole/phenol (in a ratio by weight of 50/50) at a concentration of 0.5 wt.% polyester P1 at a temperature of 25 C) and a melting point in the range from 50 to 170 C, and with the further proviso that from 0.01 to 5 mol% in relation to the molar quantity of the component (a1) used of compound D with at least three groups capable of forming esters are used to produce the polyesters P1, and other biodegradable polymers and thermoplastic moulding compounds and adhesives, biodegradable mouldings, foams and blends with starch obtainable from the polymers or moulding compounds of the invention.
-
-
-
-
-
-
-
-
-