POLYURETHANE AND ITS PRODUCTION
    1.
    发明专利

    公开(公告)号:JPH10101758A

    公开(公告)日:1998-04-21

    申请号:JP17844997

    申请日:1997-07-03

    Applicant: BASF AG

    Abstract: PROBLEM TO BE SOLVED: To obtain a polyurethane useful as a material for coating by reacting a specified polyhydric alcohol with an isocyanate. SOLUTION: This polyurethane which is suitable as a material or component of a coating material is obtained by reacting a prepolymer (a) obtained by reacting a polyhydric alcohol having more than one isocyanate-reactive hydroxyl group per molecule with an aromatic or aliphatic polyisocyanate in a ratio of the number of the isocyanatte-reactive hydroxyl groups to the number of the isocyanate groups of below 1 with an isocyanate selected from the group consisting of aromatic or aliphatic polyisocyanates (b) and a chain extender (2) obtained by reacting a polyhydric alcohol (a) with a compound (b) having an epoxy functional group and additionally an alcohol-reactive functional group, a reaction product (b) of the reaction product with an α,β-olefinically unsaturated carboxylic acid, and reacting this reaction product with an amine having a reactive prim. amino group.

    4.
    发明专利
    未知

    公开(公告)号:DE502005002887D1

    公开(公告)日:2008-04-03

    申请号:DE502005002887

    申请日:2005-07-19

    Applicant: BASF AG

    Abstract: Preparation of polyurethane-foaming substance (A) with reduced emission comprises: reacting polyisocyante with a compound (B) containing at least two reactive hydrogen atoms of isocyanates in the presence of a catalysts, where the catalyst is at least an alcohol compound (I). Preparation of polyurethane-foaming substance (A) with reduced emission comprises: reacting polyisocyanate with a compound containing at least two reactive hydrogen atoms of isocyanates in the presence of a catalyst, where the catalyst is an alcohol compound of formula (I). R1, R2 : -C aH 2a+1 or -C bH cN d; a : 1-4; b : 3-7; c : 6-14; d : 0-2; R3 : C eH fO g; e : 0-4; f : 0-8; g : 0-2; R4 : H, CH 3 or C 2H 5; and n, m : 1-5. An independent claim is also included for the polyurethane-foaming substance obtained by the method with a content of volatile organic compounds (less than 100 ppm) and condensable compounds (less than 250 ppm). [Image].

    Michael addition product useful as crosslinking agent for polyurethane

    公开(公告)号:DE19805136A1

    公开(公告)日:1999-08-12

    申请号:DE19805136

    申请日:1998-02-09

    Applicant: BASF AG

    Abstract: A Michael addition product for the crosslinking of polyurethane is prepared by mixing an acrylate with an amine. A Michael addition product (I) of formula (1a) or (1b) is prepared by mixing an acrylate of formula (2a) with an amine of formula (3a) or an acrylate of formula (2b) with an amine of formula (3b). Independent claims are included for: (i) a polyurethane (II) containing (I) or a Michael addition product prepared from ammonia and/or a 2-30 C hydrocarbon containing a primary or secondary amine group and a further group reactive with isocyanate or their mixture and/or an olefinic 4-30 C carboxyl compound as a crosslinking agent; (ii) a process for the production of (II) by mixing the crosslinking agent with the other components; and (iii) fibers, film, foam and molding compositions containing (II). R1, R3, R3', R3'', R7, R8', R8'' = H or 1-20 C hydrocarbon; R2 = (4); R4,R5R6 = 1-20 C hydrocarbon; R9I-R9VIII = H or 1-6 C hydrocarbon; D = H or an alkali; alkaline earth and/or tetraalkylammonium cation whereby the nitrogen is in the form of an anion in the presence of the cation; X = OH and/or SH; a = 0-3; b = 0-10; c = 1-4, with the provision that x has no validity with a+c=4; d = 0-10; e = 0-5; f = 0-10; g = 0-1; g+h+x = 3, with the provision that c has no validity in these cases; i = 1 or 2; j = 0-2; i+j = 1-3; k = 1-20; l = 1-20; m = 1-20; n = 1-20; o = 0-1; p = 1 or 2; q = 0 or 1; r = 1 or 2; s = 1 or 2; t = 1 or 2 with s+t=3; u = 0-20; x = 1 or 2.

    Dispersion resins for pigment coatings or formulations

    公开(公告)号:DE19626839A1

    公开(公告)日:1998-01-08

    申请号:DE19626839

    申请日:1996-07-04

    Applicant: BASF AG

    Abstract: Polymers (I), suitable as dispersion resins, are prepared by reacting polymers (II), obtained by reacting (A) compounds (III) with compounds (IX) containing an N-oxyl radical functional group, with (B) at least one compound (X) comprising the reaction product of 50-100 wt.% at least one compound (XI) and 0-50 wt.% at least one compound (XIX), in the presence of a compound (XXV) with an N-oxyl radical functional group, so that (I) comprise 10-90 wt.% (II) and 10-90 wt.% (X). (III) are chosen from (a) esters (IV) of alpha , beta -unsaturated carboxylic acids (V) and 1-25C alkyl alcohol(s) (VI), (b) esters (VII) of vinyl alcohol and 1-4C saturated carboxylic acids (VIII), (c) vinyl chloride and (d) styrene or vinyl benzene containing a 1-4C alkyl group as a ring substituent. (XI) are chosen from (a1) esters (XII) of alpha , beta -unsaturated carboxylic acids (XII) and 2-10C alkyl alcohol(s) (XIV) containing at least one polar or acidic group, (a2) amides (XVX) of alpha , beta -unsaturated carboxylic acids (XVI) and ammonia or 2-10C amines (XVII) containing at least one polar or acidic group, (a3) N-vinyl compounds (XVIII) and (a4) styrene sulphonic acid or a vinyl benzene sulphonic acid containing a 1-4C alkyl ring substituent. (XIX) are chosen from (b1) esters (XX) of alpha , beta -unsaturated carboxylic acids (XXI) and 1-25C alkyl alcohol(s) (XXII), (b2) esters (XXIII) of vinyl alcohol and 1-4C saturated carboxylic acids (XXIV), (b3) vinyl chloride and (b4) styrene or vinyl benzene containing a 1-4C alkyl ring substituent.

    Insulation board or thermal conductivity measurement reference plate

    公开(公告)号:DE19624500A1

    公开(公告)日:1998-01-02

    申请号:DE19624500

    申请日:1996-06-19

    Applicant: BASF AG

    Abstract: A device comprising at least one base plate and at least one cover plate held in a frame with the void regions containing a microcellular filler uses carbon black to colour the filler. Also claimed is preparation of the device by gluing or welding the plates and frame together. Preferably long term thermal conductivity is less than 30 mW/m.K and long term thermal conductivity stability is more than 1a (1 year). The plates and frame comprise thermoplastic or foamed plastic, preferably hard polyurethane foam with an open cell structure. Metal oxide or (preferably) silica aerogel particles with an average size of 0.001-5 mm is used as the filler.