Polycarbonate moulding material which does not form burning drips when burnt

    公开(公告)号:DE19540312A1

    公开(公告)日:1997-04-30

    申请号:DE19540312

    申请日:1995-10-28

    Applicant: BASF AG

    Abstract: Moulding materials (MM), containing (A) 1-96.5 wt% halogen- free polycarbonate(s), (B) 1-96.5 wt% halogen-free graft copolymer consisting of (b1) 40-80 wt% rubber-elastic grafting base with a Tg of below 0 deg C and (b2) 20-60 wt% grafted shell derived from (b21) 50-95 wt% vinylaromatic monomers of formula (I), in which R = H or 1-8C alkyl; R = 1-8C alkyl; n = 0, 1, 2 or 3; and/or MMA, and (b22) 5-50 wt% (meth)acrylonitrile, MMA and/or maleic anhydride, (C) 1-96.5 wt% halogen-free thermoplastic copolymer with an average mol. wt. (Mw) of less than 400,000, derived from (c1) 50-95 wt% monomer (I) and/or MMA and (c2) 5-50 wt% comonomer(s) as in (b22), (D) 0.5-30 wt% halogen-free thermoplastic copolymer with a Mw of at least 800,000 and a wide mol. wt. distribution, derived from (d1) 50-95 wt% monomer(s) (I), (d2) 5-50 wt% comonomers as in (b22) and (d3) 0-15 wt% mono-unsaturated comonomers with at least one polar functional group, (E) 1-25 wt% halogen-free phosphorus compound(s) and (F) 0-50 wt% additives. Also claimed are mouldings, film and fibres containing MM.

    Partly crosslinked polypropylene@ materials useful for fibres

    公开(公告)号:DE4422165A1

    公开(公告)日:1996-01-04

    申请号:DE4422165

    申请日:1994-06-24

    Applicant: BASF AG

    Abstract: Partly crosslinked plastic materials (A) with a melt flow index 230/2.16 of 0.1-100 g/10 minutes are obtd from: (a1) a polymer contg: (a1.1) 25-97 wt% of a copolymer of propylene with 0.1-15 wt% 2-10C alkene-1, and (a1.2) 3-75 wt% of a copolymer of propylene with 15-80 wt% 2-10C alkene-1; or (a2) a polymer contg: (a2.1) 25-97 wt% propylene homopolymer, and (a2.2) 3-75 wt% copolymer (a1.2) as above; or (a3) a propylene homopolymer with a melt flow index 230/2 of 0.1-100 g/10 minutes; or (a4) a statistical propylene copolymer contg less than 15 wt% 2-10C alkene-1 comonomer; and (b) a cpd of formula: (H2C=CR-COO)nX (I) R = H or 1-4C alkyl; X = 1-30C alkyl or 7-30C aralkyl, opt contg in-chain O and/or N atom(s); and n = 2 or 3; and these materials (A) are obtd by reacting (a1), (a2), (a3) or (a4) with cpd (b) at 180-280 deg C and 1-100 bar for a mean residence time of 0.2-10 minutes. Also claimed are: (i) a process for the prodn of (A) by reacting the above polymers with (b) at 190-260 deg C and 1-60 bar for a mean residence time of 0.2-5 minutes, pref immediately after prodn of the polymer in a mixer connected to the polymerisation reactor; and (ii) films, fibres and mouldings made from (A).

    27.
    发明专利
    未知

    公开(公告)号:AT198755T

    公开(公告)日:2001-02-15

    申请号:AT97108872

    申请日:1997-06-03

    Applicant: BASF AG

    Abstract: Ziegler-Natta type catalyst system (ZNC), containing (a) a titanium-based solid component containing compounds of Ti and magnesium, a halogen, an inorganic oxide support (IOS) and a carboxylate ester as electron donor, (b) an aluminium compound and (c) optionally another electron donor, in which the oxide (IOS) has a pH of 1-6, an average particle diameter of 5-200 microns and an average primary particle diameter of 1-20 mu m, and contains pores or channels with an average diameter of 0.1-20 mu m in amounts of 5-30 vol%. Also claimed is (i) a process for the production of ZNC by interacting components (a), (b) and (c) together at 0-150 degrees C and 1-100 bar; (ii) a process for the production of polymers of 2-20C alk-1-enes by polymerisation of the alkene (preferably propylene) and optionally other comonomers at 20-150 degrees C and 1-100 bar in presence of (ZNC); (iii) polymers of propylene obtained by this process.

    28.
    发明专利
    未知

    公开(公告)号:DE19726796A1

    公开(公告)日:1999-01-07

    申请号:DE19726796

    申请日:1997-06-24

    Applicant: BASF AG

    Abstract: Propylene polymers (I) contain a matrix of propylene homopolymer and a copolymer of propylene and other alkenes. The novelty is that the polymers satisfy certain condition(s) when separated by tacticity and comonomer distribution of the polymer chain. They are first dissolved in boiling xylene, then the solution is cooled to 25 degrees C at a rate of 10 degrees C/hour. The polymers are separated, into fractions of different solubility at increasing temperature, whilst the matrix remains undissolved on heating the cooled solution to 80 degrees C. The conditions are that the amount of matrix remaining undissolved on further heating is (i) > 20 wt.% at 112 degrees C; (ii) > 8 wt.% at 117 degrees C and/or > 1 wt.% at 122 degrees C. Also claimed are (1) a method of producing (I); and (2) films, fibres or mouldings made from (I).