    Abstract: A planetary gear retrieval system for pulling a sled at a constant velocity along an interior of a pipe, and a sled for applying a coating material to the interior of the large-diameter pipe. The planetary gear retrieval system is connected to the sled via a chain, and has a network of gears controlled by a first variable speed microcontroller. A spinner on a linear oscillating plate provided on the sled is controlled by a second variable speed microcontroller. The first and second microcontrollers are programmable to be synchronized with one another so as to pull the sled at a desired constant rate and achieve a desired number of passes of the spinner along a given length of pipe while the sled is pulled at the desired rate.

    Abstract translation: 一种行星齿轮取出系统,用于沿着管内部以恒定的速度拉动滑板,以及用于将涂料施加到大直径管内部的滑板。 行星齿轮检索系统通过链条连接到滑轨,并具有由第一变速微控制器控制的齿轮网络。 设置在滑轨上的线性振荡板上的旋转器由第二变速微控制器控制。 第一和第二微控制器可编程为彼此同步,以便以期望的恒定速率拉动滑板,并且在滑板以期望的速率被拉动时,沿着给定长度的管道实现旋转器的期望数量的通过。

    System and method for coating tubes
    47.
    发明授权
    System and method for coating tubes 有权
    涂管的系统和方法

    公开(公告)号:US08359996B2

    公开(公告)日:2013-01-29

    申请号:US12720356

    申请日:2010-03-09

    Inventor: Michael J. Horn

    Abstract: The present invention relates to coating of tubes, and more particularly to a system and method for coating and/or renovating deteriorated or pitted tubes to extend tube life and enhance performance. Using this system and method a thin coating is applied to the interior of a tube such that the coating is uniform in thickness and covers all regions of the tube. The coating material may be selected to minimize changes in heat transfer or may be selected to provide for the change in working fluid within the tube such that the working fluid does not negatively interact with the tube material.

    Abstract translation: 本发明涉及管的涂覆,更具体地说,涉及一种用于涂覆和/或改造劣化或凹陷管以延长管寿命和增强性能的系统和方法。 使用该系统和方法,将薄涂层施加到管的内部,使得涂层的厚度均匀且覆盖管的所有区域。 可以选择涂层材料以使热传递的变化最小化,或者可以选择以提供管内的工作流体的变化,使得工作流体不与管材料负相互作用。

    Method for protecting against corrosion and scale deposit and for restoring tubes of heat-exchanging equipment and device for carrying out said method
    48.
    发明授权
    Method for protecting against corrosion and scale deposit and for restoring tubes of heat-exchanging equipment and device for carrying out said method 有权
    用于防止腐蚀和结垢沉积的方法以及用于恢复热交换设备的管和用于执行所述方法的装置

    公开(公告)号:US07836844B2

    公开(公告)日:2010-11-23

    申请号:US10485580

    申请日:2002-08-06

    CPC classification number: F28F19/04 B05D7/222 Y10S118/10

    Abstract: The inventive method for protecting from corrosion and scale deposit and restoring tubes of heat-exchanging equipment consists in applying a polymeric coating on the internal surface of tubes by gradually and rotationally moving an excessive volume of polymeric material therealong and in hardening said material. A polymeric compound having an at-rest viscosity ranging from 1000 to 1200 poises and a thixotropic viscosity reduction during the displacement thereof is used as a polymeric material. The inventive device for carrying out said method comprises a loading chamber (2), a connecting washer (12), a unit for progressively displacing the polymeric material provided with spaced rigid washers (4,5,6) fixed to a metallic rod (7), an elastic screw (8) having a conical shape whereby the conicity thereof ranges from 5 to 10° on the side which is opposite in relation to the connecting washer. Said elastic screw is arranged in such a way that it is enable to perform the gradual rotation, the rotation displacement being performed at a linear speed of 0.4-1.0 m/sec and the gradual displacement being performed at a speed of 1-0.49 m/sec.

    Abstract translation: 用于防止热交换设备的腐蚀和水垢沉积和恢复管的本发明的方法在于通过在其上逐渐和旋转地移动过量体积的聚合物材料并使所述材料硬化,将聚合物涂层施加在管的内表面上。 作为聚合物材料使用具有1000至1200泊的静止粘度和其位移期间的触变粘度降低的聚合物。 用于执行所述方法的本发明的装置包括装载室(2),连接垫圈(12),用于逐渐移置聚合材料的单元,所述单元用于固定到金属杆(7)上的间隔开的刚性垫圈(4,5,6) ),具有圆锥形状的弹性螺钉(8),从而在与连接垫圈相反的一侧上其锥度为5至10°。 所述弹性螺杆以能够进行逐渐旋转的方式配置,以0.4-1.0m / sec的线速度进行旋转位移,以1-0.49m / sec的速度进行逐渐位移, 秒

    Methods of lining the internal surface of a pipe
    49.
    发明授权
    Methods of lining the internal surface of a pipe 失效
    衬管内表面的方法

    公开(公告)号:US5873390A

    公开(公告)日:1999-02-23

    申请号:US685028

    申请日:1996-07-19

    CPC classification number: F16L55/164 B05C7/08 F16L55/16 F16L55/38

    Abstract: There is provided a method of lining the internal surface of a pipe involving a larger diameter portion, said method comprising the steps of inserting a first pig into the pipe from an open end thereof, said first pig being a spherical body made of a resilient material having a diameter larger than the pipe inner diameter and having a number of grooves formed on the surface thereof for permitting air escape, injecting behind the first pig a necessary amount of resin into the pipe, inserting behind the resin a second pig into the pipe, said second pig having a diameter smaller than the pipe inner diameter such that a resin lining layer having a desired thickness may be formed on the internal surface of the pipe, providing a positive pressure and applying the positive pressure behind the second pig in the pipe, and causing the first pig, the resin and the second pig to move through the pipe along the entire length thereof by the positive pressure, so as to form a resin lining layer on the internal surface of the pipe by means of the second pig.

    Abstract translation: 提供了一种衬套包括较大直径部分的管的内表面的方法,所述方法包括以下步骤:将第一猪从其开口端插入管中,所述第一猪是由弹性材料制成的球体 其直径大于管内径,并且在其表面上形成有多个槽,用于允许空气逸出,将第一个猪后面注入必要量的树脂到管中,将第二个猪的树脂插入管中, 所述第二猪的直径小于管内径,使得可以在管的内表面上形成具有期望厚度的树脂衬层,提供正压力并将正压在第二猪后面施加在管中, 并使第一猪,树脂和第二猪沿其整个长度通过正压移动通过管,从而在其上形成树脂衬层 e通过第二只猪的管子的内表面。