금속 부재 및 세라믹 부재를 접합하는 방법
    3.
    发明公开
    금속 부재 및 세라믹 부재를 접합하는 방법 有权
    焊接金属部件和陶瓷部件的方法

    公开(公告)号:KR1020130100481A

    公开(公告)日:2013-09-11

    申请号:KR1020120021706

    申请日:2012-03-02

    Abstract: PURPOSE: A method for bonding a metal member and a ceramic member is provided to bond the metal member and the ceramic member in an atmospheric condition without an insertion metal or an adhesive. CONSTITUTION: A method for bonding a metal member and a ceramic member includes: a step of meshing or overlapping the metal member with the ceramic member; a step of placing the tool of a milling machine on a portion in which the metal member is overlapped with the ceramic member; a step of moving the tool along the portion; and a step of removing burr at a bonding surface between the metal member and the ceramic member. The metal member includes nonferrous metal and ferrous metal, and the ceramic member includes carbonized, nitrified, and oxidized ceramics. [Reference numerals] (AA) Step of meshing or overlapping the metal member with the ceramic member; (BB) Step 110; (CC) Step of placing the tool of a milling machine on a portion in which the metal member is overlapped with the ceramic member; (DD) Step 120; (EE) Step of moving the tool along the overlapped portion; (FF) Step 130; (GG) Step of removing burr at a bonding surface; (HH) Step 140

    Abstract translation: 目的:提供一种用于接合金属构件和陶瓷构件的方法,以在没有插入金属或粘合剂的情况下将金属构件和陶瓷构件在大气条件下接合。 构成:金属构件和陶瓷构件的接合方法包括:使金属构件与陶瓷构件啮合或重叠的工序; 将铣床的工具放置在金属构件与陶瓷构件重叠的部分上的步骤; 沿着该部分移动工具的步骤; 以及在金属构件和陶瓷构件之间的接合表面处去除毛刺的步骤。 金属构件包括有色金属和黑色金属,陶瓷构件包括碳化,硝化和氧化的陶瓷。 (附图标记)(AA)金属构件与陶瓷构件的啮合或重叠的步骤; (BB)步骤110; (CC)将铣床的刀具放置在金属构件与陶瓷构件重叠的部分上的步骤; (DD)步骤120; (EE)沿着重叠部分移动工具的步骤; (FF)步骤130; (GG)去除接合面上的毛刺的步骤; (HH)步骤140

    마찰교반 접합장치
    4.
    发明公开
    마찰교반 접합장치 无效
    摩擦搅拌焊接设备

    公开(公告)号:KR1020120008802A

    公开(公告)日:2012-02-01

    申请号:KR1020100069948

    申请日:2010-07-20

    Abstract: PURPOSE: An apparatus for friction stir welding is provided to prevent the adhesion between a binded material and a backing plate due to frictional heat by using aluminum nitride. CONSTITUTION: An apparatus for friction stir welding comprises a first member(20), a second member(22), a tool(10), a backing plate(30) and a contact plate. The first member and the second member each other adhere closely for friction stirring joint. A tool is inserted into the junction of the second member and the first member. The tool welds the first member and the second member through the friction stir. The backing plate supports the first member and the second member. The contact plate is inserted into the backing plate. The contact plate is inserted into the part corresponding to the junction of the second member and the first member. The contact plate is made of aluminum nitride.

    Abstract translation: 目的:提供一种用于摩擦搅拌焊接的装置,以防止由于通过使用氮化铝而产生的摩擦热而在捆扎材料和背板之间的粘合。 构成:用于摩擦搅拌焊接的装置包括第一构件(20),第二构件(22),工具(10),背板(30)和接触板。 第一构件和第二构件彼此紧密接合用于摩擦搅拌接头。 工具插入第二构件和第一构件的接合处。 该工具通过摩擦搅拌焊接第一构件和第二构件。 背板支撑第一构件和第二构件。 接触板插入背板中。 接触板被插入到与第二构件和第一构件的接合部相对应的部分中。 接触板由氮化铝制成。

    적층 커패시터 및 이의 제조방법
    10.
    发明公开
    적층 커패시터 및 이의 제조방법 有权
    多层电容器及其制造方法

    公开(公告)号:KR1020170073085A

    公开(公告)日:2017-06-28

    申请号:KR1020150181537

    申请日:2015-12-18

    Abstract: 적층커패시터가개시된다. 적층커패시터는제1 금속층및 이의일면상에배치된제1 유전체층을각각구비하는제1 박막구조체들및 이들과교대로적층되고각각제2 금속층및 이의일면상에배치된제2 유전체층구비하는제2 박막구조체들을구비하는커패시터적층구조체; 커패시터적층구조체의제1 및제2 측면상에각각배치되고제2 금속층들및 제1 금속층들과각각접촉하는제1 공통전극및 제2 공통전극을구비한다.

    Abstract translation: 公开了一种层压电容器。 根据权利要求2的层状电容器,其包括第一金属层和包含其分别设置在所述表面上的第一电介质层的第一薄膜结构,以及这些和交替层叠与每个所述第二金属层和设置在其表面上一个第二电介质层 具有薄膜结构的电容器层压结构; 分别设置在电容器2 mitje叠层结构的第一侧上设置有第一公共电极和第二公共电极,每个与所述第二金属层和第一金属层接触。

Patent Agency Ranking