Abstract:
A method for fabricating a ceramic component is disclosed. The method may comprise: 1) forming a polymer template having a shape that is an inverse of a shape of the ceramic component, 2) placing the polymer template in a mold; 3) injecting the polymer template with a ceramic slurry, 4) firing the ceramic slurry at a temperature to produce a green body, and 5) sintering the green body at an elevated temperature to provide the ceramic component.
Abstract:
A process of printing applies printing ink to the surface of a product of thermoplastic rubber compounds containing upwards of 95% mineral oil. The process uses ink compositions of resins, mineral oil, solvents, colorants, and additives. The process involves preparing a product from copolymer resins and other components, and blending an ink from copolymer resins and other components. Next, the process prints the desired multi-color image on the treated surface followed with a top coat on the surface of the substrate to protect the printed image. The top coat and ink stretch with the product so that the image remains intact. The process uses pad printing to print the image upon the surface of the product.
Abstract:
A component, the surface of which is at least partially covered with a coating, wherein the coating comprises a PVD coating arranged between a first paint layer and a second paint layer and the first paint layer forms a base coat layer on the surface and the second paint layer forms a top coat layer having a top coat thickness on the PVD coating, wherein at least the top coat layer was produced with UV-curable paint. Proceeding from the interface of the PVD coating in a region smaller than the top coat thickness, the top coat layer has a lower degree of cross-linking induced by UV light than in the part of the top coat layer connected to said region. The invention relates in particular to a method for producing such a component.
Abstract:
A method for preparing a coated substrate that includes (a) applying a photoinitiator to a surface of a substrate; (b) exposing the photoinitiator to ultraviolet or ultraviolet-visible radiation to activate the photoinitiator and form a pre-treated surface; and (c) applying a coating composition to the pre-treated substrate to form a coated substrate. The coating composition may be a nanoparticle-containing emulsion.
Abstract:
Disclosed is a multi-layer body with high weathering resistance comprising (a) a substrate layer containing at least one thermoplastic polymer (b) one cover layer on at least one side of the substrate layer, characterised in that the substrate layer further contains: (a1) at 0.02 wt. % to 0.2 wt %, at least one colorant on the basis of anthraquinone of structure (1) or (2) with structure (1), R1 and R2 standing, independently of each other, for H, OH, OR5 NH2 and NHR5, R5 being selected from alkyl, cycloalkyl, phenyl and substituted and annulated phenyls, and R3 standing for H, alkyl, alkoxy, and R4 standing for H, OH and p-methylphenyl-NH—; and with structure (2): (a2) at 0.01 wt % to 1.00 wt. %, one or a plurality of demoulders, and the cover layer consisting of a coating on the basis of polysiloxane or on the basis of polyacrylate or on the basis of polyurethane acrylate, containing at least one UV-absorber and having a layer thickness of 2-15 m.
Abstract:
Embodiments of a superhydrophobic structure comprise a substrate and a hierarchical surface structure disposed on at least one surface of the substrate, wherein the hierarchical surface structure comprises a microstructure comprising a plurality of microasperities disposed in a spaced geometric pattern on at least one surface of the substrate. The fraction of the surface area of the substrate covered by the microasperities is from between about 0.1 to about 1. The hierarchical structure comprises a nanostructure comprising a plurality of nanoasperities disposed on at least one surface of the microstructure.
Abstract:
Method for flow coating a polymeric material, wherein at least a. one component (1) is inserted at an angle of 25° to 90° relative to the floor (5) into a holder (2), b. the component (1) is coated from an upper edge (1a) with a varnish (3) and the varnish (3) is, in the meantime or thereafter, impinged on within a region of 30% of the surface of the component (1) adjacent the upper edge (1a) by a stream of air (4).
Abstract:
An aspect of the present invention relates to method of manufacturing a hard coat film, wherein the hard coat film comprises a plastic substrate and a hard coat layer, the method comprises forming the hard coat layer by subjecting a photopolymerizable hard coating composition to photopolymerization processing, and the photopolymerizable hard coating composition comprises a radical polymerizable compound having two or more radical polymerizable groups selected from the group consisting of acryloyloxy groups, acryloyl groups, methacryloyloxy groups, and methacryloyl groups per molecule, a cationic polymerizable compound, a radical photopolymerization initiator, and a cationic photopolymerization initiator.
Abstract:
Method for flow coating a polymeric material, wherein a. at least one component (1) is inserted at an angle of 25° to 90° relative to the floor (5) into a holder (2), and b. the component (1) is coated from the upper edge (1a) with a varnish (3), containing 10 wt.-% to 30 wt.-% of 4-methyl-2-pentanone and/or derivatives thereof.
Abstract:
A tire has a coating with a quadlayer or multiple quadlayers, and a method produces the same. In an embodiment, the method for coating a rubber substrate includes exposing the rubber substrate to a first cationic solution to produce a first cationic layer on the rubber substrate. The method also includes exposing the first cationic layer to a first anionic solution to produce a first anionic layer on the first cationic layer. In addition, the method includes exposing the first anionic layer to a second cationic solution to produce a second cationic layer on the first anionic layer. The method further includes exposing the second cationic layer to a second anionic solution to produce a second anionic layer on the second cationic layer. A quadlayer includes the first cationic layer, the first anionic layer, the second cationic layer, and the second anionic layer. The coating includes the quadlayer.